Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 5-240 mm

Mechanical

PropertyValueComment

Elongation

8 %

Show Supplier Material materials with Elongation of 8 %

min.

Hardness, Brinell

331.0 - 392.0 [-]

Show Supplier Material materials with Hardness, Brinell of 331.0 - 392.0 [-]

Tensile strength

1070 MPa

Show Supplier Material materials with Tensile strength of 1070 MPa

min.

Yield strength

1000.0 MPa

Show Supplier Material materials with Yield strength of 1000.0 MPa

min., RP02

Chemical properties

PropertyValueComment

Carbon

0.07 %

Show Supplier Material materials with Carbon of 0.07 %

max.

Chromium

15.0 - 15.5 %

Show Supplier Material materials with Chromium of 15.0 - 15.5 %

Copper

2.5 - 4.5 %

Show Supplier Material materials with Copper of 2.5 - 4.5 %

Manganese

1.0 %

Show Supplier Material materials with Manganese of 1.0 %

max.

Molybdenum

0.5 %

Show Supplier Material materials with Molybdenum of 0.5 %

max.

Nickel

3.0 - 5.5 %

Show Supplier Material materials with Nickel of 3.0 - 5.5 %

Niobium

0.005 %

Show Supplier Material materials with Niobium of 0.005 %

max.

Phosphorus

0.03 %

Show Supplier Material materials with Phosphorus of 0.03 %

max.

Silicon

1.0 %

Show Supplier Material materials with Silicon of 1.0 %

max.

Sulfur

0.015 %

Show Supplier Material materials with Sulfur of 0.015 %

max.

Technological properties

Property
Application areas

Aerospace

Processing history

Hardened