1.4713

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Remy Stahl.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 100 mm

Mechanical

PropertyValueComment

Elongation

25 %

Show Supplier Material materials with Elongation of 25 %

min.

Hardness, Brinell

192 [-]

Show Supplier Material materials with Hardness, Brinell of 192 [-]

max.

Tensile strength

420.0 - 620.0 MPa

Show Supplier Material materials with Tensile strength of 420.0 - 620.0 MPa

Yield strength

220.0 MPa

Show Supplier Material materials with Yield strength of 220.0 MPa

min., RP02

Chemical properties

PropertyValueComment

Carbon

0.08 %

Show Supplier Material materials with Carbon of 0.08 %

max.

Chromium

17.0 - 19.0 %

Show Supplier Material materials with Chromium of 17.0 - 19.0 %

Manganese

2.0 %

Show Supplier Material materials with Manganese of 2.0 %

max.

Nickel

9.0 - 12.0 %

Show Supplier Material materials with Nickel of 9.0 - 12.0 %

Niobium

1.0 %

Show Supplier Material materials with Niobium of 1.0 %

max.

Phosphorus

0.045 %

Show Supplier Material materials with Phosphorus of 0.045 %

max.

Silicon

1.0 %

Show Supplier Material materials with Silicon of 1.0 %

max.

Sulfur

0.015 %

Show Supplier Material materials with Sulfur of 0.015 %

max.

Technological properties

Property
Application areas

Plant construction, Apparatus engineering, Power Generation, Mechanical Engineering, Power plants, Plate girder and pipes in furnace construction, in apparatus engineering for air preheaters, Superheater suspensions, Annealing hoods, Rails, Barrels

Processing history

Annealed