Dimension

PropertyValue

Mechanical

PropertyValue

Chemical properties

Property

Aluminium

0.04 %

max.

Carbon

0.08 - 0.12 %

Chromium

8 - 9.5 %

Iron

Balance

Manganese

0.3 - 0.6 %

Molybdenum

0.85 - 1.05 %

Nickel

0.4 %

max.

Nitrogen

0.03 - 0.07 %

Phosphorus

0.03 %

max.

Silicon

0.5 %

max.

Sulfur

0.015 %

max.

Vanadium

0.18 - 0.25 %

Technological properties