Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 6-500 mm

Mechanical

PropertyValueComment

Elongation

12 %

Show Supplier Material materials with Elongation of 12 %

min.

Hardness, Brinell

270.0 - 311.0 [-]

Show Supplier Material materials with Hardness, Brinell of 270.0 - 311.0 [-]

Tensile strength

900.0 - 1050.0 MPa

Show Supplier Material materials with Tensile strength of 900.0 - 1050.0 MPa

Yield strength

750.0 MPa

Show Supplier Material materials with Yield strength of 750.0 MPa

min., RP02

Chemical properties

PropertyValueComment

Boron

0.0015 - 0.005 %

Show Supplier Material materials with Boron of 0.0015 - 0.005 %

Carbon

0.04 %

Show Supplier Material materials with Carbon of 0.04 %

max.

Chromium

10.0 - 18.0 %

Show Supplier Material materials with Chromium of 10.0 - 18.0 %

Manganese

2.0 %

Show Supplier Material materials with Manganese of 2.0 %

max.

Molybdenum

2.0 - 3.0 %

Show Supplier Material materials with Molybdenum of 2.0 - 3.0 %

Nickel

12.0 - 14.0 %

Show Supplier Material materials with Nickel of 12.0 - 14.0 %

Nitrogen

0.1 - 0.18 %

Show Supplier Material materials with Nitrogen of 0.1 - 0.18 %

Phosphorus

0.035 %

Show Supplier Material materials with Phosphorus of 0.035 %

max.

Silicon

0.75 %

Show Supplier Material materials with Silicon of 0.75 %

max.

Sulfur

0.015 %

Show Supplier Material materials with Sulfur of 0.015 %

max.

Technological properties

Property
Application areas

Connecting parts, High temperature resistant components, Nuts, Screws

Processing history

Quenched and Tempered