1.4980

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Remy Stahl.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 6.5-310 mm - Hexagonal Bar: 13- 60 mm

Mechanical

PropertyValueComment

Elongation

16 %

Show Supplier Material materials with Elongation of 16 %

min.

Hardness, Brinell

248.0 - 341.0 [-]

Show Supplier Material materials with Hardness, Brinell of 248.0 - 341.0 [-]

Tensile strength

900.0 - 1150.0 MPa

Show Supplier Material materials with Tensile strength of 900.0 - 1150.0 MPa

Yield strength

600.0 MPa

Show Supplier Material materials with Yield strength of 600.0 MPa

min., RP02

Chemical properties

PropertyValueComment

Carbon

0.04 - 0.1 %

Show Supplier Material materials with Carbon of 0.04 - 0.1 %

Chromium

15.0 - 17.0 %

Show Supplier Material materials with Chromium of 15.0 - 17.0 %

Manganese

1.5 %

Show Supplier Material materials with Manganese of 1.5 %

max.

Nickel

24.0 - 27.0 %

Show Supplier Material materials with Nickel of 24.0 - 27.0 %

Phosphorus

0.035 %

Show Supplier Material materials with Phosphorus of 0.035 %

max.

Silicon

0.3 - 0.6 %

Show Supplier Material materials with Silicon of 0.3 - 0.6 %

Sulfur

0.015 %

Show Supplier Material materials with Sulfur of 0.015 %

max.

Titanium

0.0001 %

Show Supplier Material materials with Titanium of 0.0001 %

max.

Technological properties

Property
Application areas

Power plant engineering, Mechanical Engineering, Power Generation, Parts for gas turbines and engines like runners, discs, shafts, screws, extension rings, fittings, housings

Processing history

Hardened