Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 10.68-100 mm

Mechanical

PropertyValue

Tensile strength

530.0 - 710.0 MPa

Show Supplier Material materials with Tensile strength of 530.0 - 710.0 MPa

Chemical properties

PropertyValueComment

Boron

0.05 - 0.1 %

Show Supplier Material materials with Boron of 0.05 - 0.1 %

Carbon

0.04 - 0.1 %

Show Supplier Material materials with Carbon of 0.04 - 0.1 %

Chromium

13.5 - 17.5 %

Show Supplier Material materials with Chromium of 13.5 - 17.5 %

Manganese

1.5 %

Show Supplier Material materials with Manganese of 1.5 %

max.

Molybdenum

1.6 - 2.0 %

Show Supplier Material materials with Molybdenum of 1.6 - 2.0 %

Nickel

15.5 - 17.5 %

Show Supplier Material materials with Nickel of 15.5 - 17.5 %

Niobium

1.2 %

Show Supplier Material materials with Niobium of 1.2 %

max.

Phosphorus

0.045 %

Show Supplier Material materials with Phosphorus of 0.045 %

max.

Silicon

0.3 - 0.6 %

Show Supplier Material materials with Silicon of 0.3 - 0.6 %

Sulfur

0.03 %

Show Supplier Material materials with Sulfur of 0.03 %

max.

Technological properties

Property
Application areas

Connecting parts, Mechanical Engineering, Components in machines and apparatus engineering, Cooling machine parts and similarly claimed parts for temperatures to -150°C

Processing history

Quenched and Tempered