1.6909

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Remy Stahl.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 14.52-52.14 mm

Mechanical

PropertyValueComment

Elongation

22 %

Show Supplier Material materials with Elongation of 22 %

min.

Tensile strength

830.0 - 1080.0 MPa

Show Supplier Material materials with Tensile strength of 830.0 - 1080.0 MPa

Yield strength

690.0 MPa

Show Supplier Material materials with Yield strength of 690.0 MPa

min., RP02

Chemical properties

PropertyValueComment

Aluminium

0.02 - 0.05 %

Show Supplier Material materials with Aluminium of 0.02 - 0.05 %

Carbon

0.18 - 0.25 %

Show Supplier Material materials with Carbon of 0.18 - 0.25 %

Chromium

1.2 - 1.5 %

Show Supplier Material materials with Chromium of 1.2 - 1.5 %

Manganese

0.3 - 0.5 %

Show Supplier Material materials with Manganese of 0.3 - 0.5 %

Molybdenum

0.25 - 0.5 %

Show Supplier Material materials with Molybdenum of 0.25 - 0.5 %

Nickel

3.4 - 4.0 %

Show Supplier Material materials with Nickel of 3.4 - 4.0 %

Phosphorus

0.02 %

Show Supplier Material materials with Phosphorus of 0.02 %

max.

Silicon

0.15 - 0.4 %

Show Supplier Material materials with Silicon of 0.15 - 0.4 %

Sulfur

0.01 %

Show Supplier Material materials with Sulfur of 0.01 %

max.

Technological properties

Property
Application areas

Connecting parts

Processing history

Strain Hardened