PropertyValue

Chemical properties

Property

Carbon

0.26 - 0.34 %

Chromium

1.8 - 2.2 %

Iron

Balance

Manganese

0.3 - 0.6 %

Molybdenum

0.3 - 0.5 %

Nickel

1.8 - 2.2 %

Phosphorus

0.03 %

max.

Silicon

0.4 %

max.

Sulfur

0.035 %

Technological properties

Property
Application areas

Mechanical Engineering, Tool technology, Automotive engineering

Processing history

Annealed and Forged