Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 14-52 mm

Chemical properties

PropertyValueComment

Carbon

0.17 - 0.25 %

Show Supplier Material materials with Carbon of 0.17 - 0.25 %

Chromium

1.2 - 1.5 %

Show Supplier Material materials with Chromium of 1.2 - 1.5 %

Manganese

0.4 - 0.8 %

Show Supplier Material materials with Manganese of 0.4 - 0.8 %

Molybdenum

0.55 - 0.8 %

Show Supplier Material materials with Molybdenum of 0.55 - 0.8 %

Nickel

0.6 %

Show Supplier Material materials with Nickel of 0.6 %

max.

Phosphorus

0.025 %

Show Supplier Material materials with Phosphorus of 0.025 %

max.

Silicon

0.4 %

Show Supplier Material materials with Silicon of 0.4 %

max.

Sulfur

0.03 %

Show Supplier Material materials with Sulfur of 0.03 %

Vanadium

0.2 - 0.35 %

Show Supplier Material materials with Vanadium of 0.2 - 0.35 %

Technological properties

Property
Application areas

Mechanical Engineering, Apparatus engineering

Processing history

Annealed and Forged