Carbon powders and graphite powders are the basis for cost efficient serial production of carbon and graphite based components.


The porous bodies are bonded with chemically and thermally stable duroplastic binder systems - all with help of SGL Carbon’s established processes and know-how.


The highly porous carbon structure of CARBOPRINT C is an ideal basis for post-processing, such as infiltration with silicon or impregnation with polymers.


The advantages of CARBOPRINT® are:

  • Lightweight - low density & open porosity
  • Form stable at high temperatures
  • Freedom of (material) design
  • Further post processing such as thermal treatment and densification possible on demand

This material data has been provided by SGL Carbon.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

1 g/cm³

Show Supplier Material materials with Density of 1 g/cm³

Porosity

open porosity

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

2 GPa

Show Supplier Material materials with Elastic modulus of 2 GPa

Flexural strength

23.0 °C

5 MPa

Show Supplier Material materials with Flexural strength of 5 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

200.0 °C

5.5E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 5.5E-6 1/K

Thermal conductivity

23.0 °C

1 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 1 W/(m·K)

max

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

0.13 Ω·m

Show Supplier Material materials with Electrical resistivity of 0.13 Ω·m

Technological properties

Property
Processing methods

The CARBOPRINT family combines our comprehensive carbon material know-how with additive manufacturing technology. In addition, our broad base of post-processing capabilities, such as resin or silicon infiltration, delivers innovative material solutions for your applications. This set of competencies and capabilities is a unique starting point for rapid and economic production of prototypes and small series of carbon based components for various industries such as glass, metal and chemicals, as well as high-temperature and mechanical applications.