Ceramic Carbon Composite CARBOPRINT® Si2

Want to keep this datasheet? Save it now in your required format

Description

Ceramic carbon composites provide ideal properties where it comes to reliable function and longevity in harsh environments and at high temperatures.


We bring decades of experience with ceramic composites to additive manufacturing in order to provide our customers the opportunity to realize almost any design with ceramic carbon composites. CARBOPRINT Si components are made by siliconizing CARBOPRINT C bodies.


The advantages of CARBOPRINT® Si are:

  • Low weight due to low density
  • High thermal shock resistance
  • High bending strength
  • High wear resistance

This material data has been provided by SGL Carbon.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

2.4 g/cm³

Show Supplier Material materials with Density of 2.4 g/cm³

Porosity

0.1 %

Show Supplier Material materials with Porosity of 0.1 %

open porosity, max

Mechanical

PropertyValue

Elastic modulus

95 GPa

Show Supplier Material materials with Elastic modulus of 95 GPa

Flexural strength

75 MPa

Show Supplier Material materials with Flexural strength of 75 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

200 °C

0.000003 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.000003 1/K

Thermal conductivity

60 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 60 W/(m·K)

Electrical

PropertyValue

Electrical resistivity

0.0001 Ω·m

Show Supplier Material materials with Electrical resistivity of 0.0001 Ω·m

Technological properties

Property
Processing methods

The CARBOPRINT family combines our comprehensive carbon material know-how with additive manufacturing technology. In addition, our broad base of post-processing capabilities, such as resin or silicon infiltration, delivers innovative material solutions for your applications. This set of competencies and capabilities is a unique starting point for rapid and economic production of prototypes and small series of carbon based components for various industries such as glass, metal and chemicals, as well as high-temperature and mechanical applications.