SIGRAFINE® Isostatic graphites R4810

Want to keep this datasheet? Save it now in your required format

Description

SIGRAFINE® Isostatic graphite is an ultra-fine grain graphite used for applications where the mechanical properties of other fine grain graphites are inadequate. The term "Isostatic Graphite" stands for isostatically molded graphite. This means that the raw material mixture is compressed into rectangular or round blocks in a so called Cold-Isostatic-Press (CIP). Compared to other technologies such as extrusion or vibration molding, this technology can produce the most isotropic form of artificial graphite. In addition, isostatic graphite generally tends to have the smallest grain sizes of all artificial graphites. Typical properties of the material:


  • Extremely high thermal and chemical resistance
  • Excellent thermal shock resistance
  • High electrical conductivity
  • High thermal conductivity
  • Increasing strength with rising temperature
  • Easy to machine
  • Can be produced with very high purity < 5 ppm
  • This material data has been provided by SGL Carbon.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyTemperatureValueComment

    Bulk density

    1.82 g/cm³

    Show Supplier Material materials with Bulk density of 1.82 g/cm³

    Grain size

    20.0 μm

    Show Supplier Material materials with Grain size of 20.0 μm

    Permeability coefficient

    20 °C

    0.3 cm²/s

    Show Supplier Material materials with Permeability coefficient of 0.3 cm²/s

    Porosity

    11.0 %

    Show Supplier Material materials with Porosity of 11.0 %

    open porosity

    Mechanical

    PropertyValueComment

    Compressive strength

    100 MPa

    Show Supplier Material materials with Compressive strength of 100 MPa

    Elastic modulus

    10.5 GPa

    Show Supplier Material materials with Elastic modulus of 10.5 GPa

    Dynamic Modulus

    Flexural strength

    45 MPa

    Show Supplier Material materials with Flexural strength of 45 MPa

    Hardness, Rockwell

    95.0 [-]

    Show Supplier Material materials with Hardness, Rockwell of 95.0 [-]

    10/100

    Thermal

    PropertyTemperatureValueComment

    Ash content

    0.005 %

    Show Supplier Material materials with Ash content of 0.005 %

    Coefficient of thermal expansion

    4.1e-06 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 4.1e-06 1/K

    @20-200°C

    Thermal conductivity

    20 °C

    140 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 140 W/(m·K)

    Technological properties

    Property
    Application areas

    Metallurgical applications e.g. continuous casting, crucibles, sintering molds, etc.

    Processing methods

    Isostatically pressed