SIGRAFINE® isostatic graphites R6710

Want to keep this datasheet? Save it now in your required format

Description

SIGRAFINE® Isostatic graphite is an ultra-fine grain graphite used for electronic applications where the mechanical properties of other fine grain graphites are inadequate. The term "Isostatic Graphite" stands for isostatically molded graphite. This means that the raw material mixture is compressed into rectangular or round blocks in a so called Cold-Isostatic-Press (CIP). Compared to other technologies such as extrusion or vibration molding, this technology can produce the most isotropic form of artificial graphite. In addition, isostatic graphite generally tends to have the smallest grain sizes of all artificial graphites. Typical properties of the material:


  • Extremely high thermal and chemical resistance
  • Excellent thermal shock resistance
  • High electrical conductivity
  • High thermal conductivity
  • Increasing strength with rising temperature
  • Easy to machine
  • Can be produced with very high purity < 5 ppm
  • This material data has been provided by SGL Carbon.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyValueComment

    Bulk density

    1.88 g/cm³

    Show Supplier Material materials with Bulk density of 1.88 g/cm³

    Grain size

    3.0 μm

    Show Supplier Material materials with Grain size of 3.0 μm

    Permeability coefficient

    0.01 cm²/s

    Show Supplier Material materials with Permeability coefficient of 0.01 cm²/s

    Porosity

    10.0 %

    Show Supplier Material materials with Porosity of 10.0 %

    open porosity

    Mechanical

    PropertyValueComment

    Compressive strength

    170 MPa

    Show Supplier Material materials with Compressive strength of 170 MPa

    Elastic modulus

    13.5 GPa

    Show Supplier Material materials with Elastic modulus of 13.5 GPa

    Dynamic Modulus

    Flexural strength

    85 MPa

    Show Supplier Material materials with Flexural strength of 85 MPa

    Hardness, Rockwell

    105.0 [-]

    Show Supplier Material materials with Hardness, Rockwell of 105.0 [-]

    5/100

    Thermal

    PropertyTemperatureValueComment

    Ash content

    0.0005 %

    Show Supplier Material materials with Ash content of 0.0005 %

    depending on the code, it can also be less than 5 ppm

    0.003 %

    Show Supplier Material materials with Ash content of 0.003 %

    depending on the code, it can also be less than 5 ppm

    Coefficient of thermal expansion

    4.7e-06 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 4.7e-06 1/K

    @20-200°C

    Thermal conductivity

    20 °C

    100 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 100 W/(m·K)

    Electrical

    PropertyValue

    Electrical resistivity

    1.3000000000000001e-05 Ω·m

    Show Supplier Material materials with Electrical resistivity of 1.3000000000000001e-05 Ω·m

    Chemical properties

    PropertyValueComment

    Aluminium

    1e-06 - 5e-06 %

    Show Supplier Material materials with Aluminium of 1e-06 - 5e-06 %

    depending on the code, it can also be less

    Boron

    2e-06 - 1e-05 %

    Show Supplier Material materials with Boron of 2e-06 - 1e-05 %

    depending on the code, it can also be less

    Calcium

    1e-06 - 2e-05 %

    Show Supplier Material materials with Calcium of 1e-06 - 2e-05 %

    depending on the code

    Chromium

    1e-06 - 2e-06 %

    Show Supplier Material materials with Chromium of 1e-06 - 2e-06 %

    depending on the code, it can also be less

    Cobalt

    1e-06 - 2e-06 %

    Show Supplier Material materials with Cobalt of 1e-06 - 2e-06 %

    depending on the code, it can also be less

    Copper

    1e-06 - 2e-06 %

    Show Supplier Material materials with Copper of 1e-06 - 2e-06 %

    depending on the code, it can also be less

    Iron

    2e-06 - 5e-05 %

    Show Supplier Material materials with Iron of 2e-06 - 5e-05 %

    depending on the code

    Magnesium

    1e-06 - 1e-05 %

    Show Supplier Material materials with Magnesium of 1e-06 - 1e-05 %

    depending on the code

    Manganese

    1e-06 %

    Show Supplier Material materials with Manganese of 1e-06 %

    max.

    Nickel

    1e-06 - 0.0001 %

    Show Supplier Material materials with Nickel of 1e-06 - 0.0001 %

    depending on the code, it can also be less

    Phosphorus

    2e-06 - 1e-05 %

    Show Supplier Material materials with Phosphorus of 2e-06 - 1e-05 %

    depending on the code, it can also be less

    Silicon

    0.0001 - 0.0002 %

    Show Supplier Material materials with Silicon of 0.0001 - 0.0002 %

    depending on the code, it can also be less

    Titanium

    1e-06 - 2e-05 %

    Show Supplier Material materials with Titanium of 1e-06 - 2e-05 %

    depending on the code

    Vanadium

    1e-06 - 5e-05 %

    Show Supplier Material materials with Vanadium of 1e-06 - 5e-05 %

    depending on the code

    Technological properties

    Property
    Processing methods

    Isostatically pressed