Description

Resin bonded specialty graphite with temperature resistance up to 180°C

This material data has been provided by SGL Carbon.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Bulk density

1.73 g/cm³

Show Supplier Material materials with Bulk density of 1.73 g/cm³

DIN IEC 60413/204

Mechanical

PropertyValueComment

Compressive strength

120 MPa

Show Supplier Material materials with Compressive strength of 120 MPa

DIN 51910

Elastic modulus

22 GPa

Show Supplier Material materials with Elastic modulus of 22 GPa

DIN 51915

Flexural strength

80 MPa

Show Supplier Material materials with Flexural strength of 80 MPa

DIN IEC 60413/501

Hardness, Rockwell

80.0 [-]

Show Supplier Material materials with Hardness, Rockwell of 80.0 [-]

5/100; DIN IEC 60413/303

Thermal

PropertyValueComment

Coefficient of thermal expansion

1.1e-05 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.1e-05 1/K

@20-150°C; DIN 51909

Thermal conductivity

6 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 6 W/(m·K)

DIN 51908

Technological properties

Property
Application areas

Vanes for dry running compressors and vacuum pumps up to 180°C

Processing methods

Hot moulded