SIGRABOND® Chemical CFRP for components and assemblies

Want to keep this datasheet? Save it now in your required format

This material data has been provided by SGL Carbon.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

1.4 g/cm³

Show Supplier Material materials with Density of 1.4 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

44 GPa

Show Supplier Material materials with Elastic modulus of 44 GPa

Failure Strain

23.0 °C

1.2 %

Show Supplier Material materials with Failure Strain of 1.2 %

Flexural modulus

23.0 °C

50 GPa

Show Supplier Material materials with Flexural modulus of 50 GPa

Flexural strength

23.0 °C

400 MPa

Show Supplier Material materials with Flexural strength of 400 MPa

Tensile strength

23.0 °C

570 MPa

Show Supplier Material materials with Tensile strength of 570 MPa

Thermal

PropertyValue

Max service temperature

160 °C

Show Supplier Material materials with Max service temperature of 160 °C

Max service temperature, inert

160 °C

Show Supplier Material materials with Max service temperature, inert of 160 °C

Technological properties

Property
Application areas

Components and assemblies based on plate material (liquid distributors, collectors, support grids, retainers)