SIGRABOND® Chemical CFRC for components and assemblies

Want to keep this datasheet? Save it now in your required format

This material data has been provided by SGL Carbon.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.5 g/cm³

Show Supplier Material materials with Density of 1.5 g/cm³

Mechanical

PropertyValue

Elastic modulus

65 GPa

Show Supplier Material materials with Elastic modulus of 65 GPa

Failure Strain

0.4 %

Show Supplier Material materials with Failure Strain of 0.4 %

Flexural modulus

75 GPa

Show Supplier Material materials with Flexural modulus of 75 GPa

Flexural strength

340 MPa

Show Supplier Material materials with Flexural strength of 340 MPa

Tensile strength

270.0 MPa

Show Supplier Material materials with Tensile strength of 270.0 MPa

Thermal

PropertyValueComment

Max service temperature

300.0 °C

Show Supplier Material materials with Max service temperature of 300.0 °C

1000 °C

Show Supplier Material materials with Max service temperature of 1000 °C

Inert

Technological properties

Property
Application areas

Components and assemblies based on plate material (liquid distributors, collectors, support grids, retainers)