ABS H2108-10 BK

Alternative and trade names
ESD ABS H2108-10 BK
Want to keep this datasheet? Save it now in your required format

Description

Acrylonitrile Butadiene Styrene (ABS) resin with carbon black added for ESD protection.

This material data has been provided by Dongguan SUGO Plastics Technology.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueTemperatureComment

Density

1.09 g/cm³

Show Supplier Material materials with Density of 1.09 g/cm³ at 23.0 °C

23.0 °C

ASTM D792

Mechanical

PropertyValueTemperatureComment

Elongation

9 %

Show Supplier Material materials with Elongation of 9 % at 23.0 °C

23.0 °C

ASTM D638

Flexural modulus

1.5 GPa

Show Supplier Material materials with Flexural modulus of 1.5 GPa at 23.0 °C

23.0 °C

ASTM D790

Flexural strength

47 MPa

Show Supplier Material materials with Flexural strength of 47 MPa at 23.0 °C

23.0 °C

ASTM D790

Impact strength, Izod notched, ASTM

10.2 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 10.2 J/m at 23.0 °C

23.0 °C

ASTM D256

Tensile strength

28 MPa

Show Supplier Material materials with Tensile strength of 28 MPa at 23.0 °C

23.0 °C

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

83 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 83 °C

ASTM D648

Electrical

PropertyValueTemperatureComment

Surface resistivity

1.00E+7 - 1.00E+10 Ω/sq

Show Supplier Material materials with Surface resistivity of 1.00E+7 - 1.00E+10 Ω/sq at 23.0 °C

23.0 °C

ASTM D257

Rheological Properties

PropertyValueTemperatureComment

Melt mass-flow rate

3.72 g/10min

Show Supplier Material materials with Melt mass-flow rate of 3.72 g/10min

ASTM D1238, 230°C/5kg

Shrinkage

0.9 %

Show Supplier Material materials with Shrinkage of 0.9 % at 23.0 °C

23.0 °C

ASTM D1238, Mold Shrinkage

Technological properties

Property
Application areas

Hard drive and memory fixtures, Computer work surfaces, ESD circular disc, ESD protection board, ESD electric & housing spare parts, Electric accessories

Certifications

RoHS

Color

Black

Processing methods

Injection molding - Drying time: 4hrs, temperature: 85°C - injection temperature: 200-230°C