ABS H7113 TG

Alternative and trade names
ESD ABS H7113 TG
Want to keep this datasheet? Save it now in your required format

Description

Acrylonitrile Butadiene Styrene (ABS) resin with permanent antistatic agent agent for long lasting ESD protection exhibiting high toughness.

This material data has been provided by Dongguan SUGO Plastics Technology.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.05 g/cm³

Show Supplier Material materials with Density of 1.05 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

13 %

Show Supplier Material materials with Elongation of 13 %

ASTM D638

Flexural modulus

23.0 °C

2.1 GPa

Show Supplier Material materials with Flexural modulus of 2.1 GPa

ASTM D790

Flexural strength

23.0 °C

65 MPa

Show Supplier Material materials with Flexural strength of 65 MPa

ASTM D790

Impact strength, Izod notched, ASTM

23.0 °C

630 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 630 J/m

ASTM D256

Tensile strength

23.0 °C

33 MPa

Show Supplier Material materials with Tensile strength of 33 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

85 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 85 °C

ASTM D648

Electrical

PropertyTemperatureValueComment

Surface resistivity

23.0 °C

1.00E+8 - 1.00E+10 Ω/sq

Show Supplier Material materials with Surface resistivity of 1.00E+8 - 1.00E+10 Ω/sq

ASTM D257

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

19 g/10min

Show Supplier Material materials with Melt mass-flow rate of 19 g/10min

ASTM D1238, 230°C/5kg

Shrinkage

23.0 °C

0.9 %

Show Supplier Material materials with Shrinkage of 0.9 %

ASTM D1238, Mold Shrinkage

Technological properties

Property
Application areas

Hard drive and memory fixtures, Computer work surfaces, ESD circular disc, ESD protection board, ESD electric & housing spare parts, Electric accessories

Certifications

RoHS

Color

Natrual color

Processing methods

Injection molding - Drying time: 4hrs, temperature: 85°C - injection temperature: 180-220°C