General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 1.06 g/cm³ Show Supplier Material materials with Density of 1.06 g/cm³ at 23.0 °C | 23.0 °C | ASTM D792 |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elongation | 31 % Show Supplier Material materials with Elongation of 31 % at 23.0 °C | 23.0 °C | ASTM D638 |
Flexural modulus | 1.26 GPa Show Supplier Material materials with Flexural modulus of 1.26 GPa at 23.0 °C | 23.0 °C | ASTM D790 |
Flexural strength | 52 MPa Show Supplier Material materials with Flexural strength of 52 MPa at 23.0 °C | 23.0 °C | ASTM D790 |
Impact strength, Izod notched, ASTM | 21 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 21 J/m at 23.0 °C | 23.0 °C | ASTM D256 |
Tensile strength | 37 MPa Show Supplier Material materials with Tensile strength of 37 MPa at 23.0 °C | 23.0 °C | ASTM D638 |
Thermal
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 85 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 85 °C | ASTM D648 |
Electrical
Property | Value | Temperature | Comment |
---|---|---|---|
Surface resistivity | 1.00E+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+10 Ω/sq at 23.0 °C | 23.0 °C | ASTM D257 |
Rheological Properties
Property | Value | Temperature | Comment |
---|---|---|---|
Melt mass-flow rate | 19.5 g/10min Show Supplier Material materials with Melt mass-flow rate of 19.5 g/10min | ASTM D1238, 230°C/5kg | |
Shrinkage | 0.81 % Show Supplier Material materials with Shrinkage of 0.81 % at 23.0 °C | 23.0 °C | ASTM D1238, Mold Shrinkage |
Technological properties
Property | ||
---|---|---|
Application areas | Hard drive and memory fixtures, Computer work surfaces, ESD circular disc, ESD protection board, ESD electric & housing spare parts, Electric accessories | |
Certifications | RoHS | |
Color | Black | |
Processing methods | Injection molding - Drying time: 4hrs, temperature: 85°C - injection temperature: 180-220°C |