Description

Polyetherether Ketone (PEEK) compound filled with carbon fiber for ESD protection.

This material data has been provided by Dongguan SUGO Plastics Technology.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueTemperatureComment

Density

1.24 g/cm³

Show Supplier Material materials with Density of 1.24 g/cm³ at 23.0 °C

23.0 °C

ASTM D792

Mechanical

PropertyValueTemperatureComment

Elongation

25 %

Show Supplier Material materials with Elongation of 25 % at 23.0 °C

23.0 °C

ASTM D638

Flexural modulus

2.03 GPa

Show Supplier Material materials with Flexural modulus of 2.03 GPa at 23.0 °C

23.0 °C

ASTM D790

Flexural strength

86 MPa

Show Supplier Material materials with Flexural strength of 86 MPa at 23.0 °C

23.0 °C

ASTM D790

Impact strength, Izod notched, ASTM

30.5 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 30.5 J/m at 23.0 °C

23.0 °C

ASTM D256, 3.2mm

Tensile strength

49 MPa

Show Supplier Material materials with Tensile strength of 49 MPa at 23.0 °C

23.0 °C

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

120 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 120 °C

ASTM D648

Electrical

PropertyValueTemperatureComment

Surface resistivity

1000 - 100000 Ω/sq

Show Supplier Material materials with Surface resistivity of 1000 - 100000 Ω/sq at 23.0 °C

23.0 °C

ASTM D257

Rheological Properties

PropertyValueTemperatureComment

Melt mass-flow rate

9.8 g/10min

Show Supplier Material materials with Melt mass-flow rate of 9.8 g/10min

ASTM D1238, 230°C/5kg

Shrinkage

0.25 %

Show Supplier Material materials with Shrinkage of 0.25 % at 23.0 °C

23.0 °C

ASTM D1238, Mold Shrinkage

Technological properties

Property
Certifications

RoHS

Color

Black

Fillers

Carbon Fiber

Processing methods

Injection molding - Drying time: 4-5hrs, temperature: 160°C - Mold temperature:180-210°C - injection temperature: 360-390°C