ABS 6120 TP

Alternative and trade names
ESD ABS 6120 TP
Want to keep this datasheet? Save it now in your required format

Description

Transparent Acrylonitrile Butadiene Styrene (ABS) resin with permanent antistatic agent agent forlong lasting ESD protection.

This material data has been provided by Dongguan SUGO Plastics Technology.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.11 g/cm³

Show Supplier Material materials with Density of 1.11 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

40 %

Show Supplier Material materials with Elongation of 40 %

ASTM D638

Flexural modulus

23.0 °C

1.3 GPa

Show Supplier Material materials with Flexural modulus of 1.3 GPa

ASTM D790

Flexural strength

23.0 °C

60 MPa

Show Supplier Material materials with Flexural strength of 60 MPa

ASTM D790

Impact strength, Izod notched, ASTM

23.0 °C

14 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 14 J/m

ASTM D256

Tensile strength

23.0 °C

36.6 MPa

Show Supplier Material materials with Tensile strength of 36.6 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

82 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 82 °C

ASTM D648

Electrical

PropertyTemperatureValueComment

Surface resistivity

23.0 °C

1.00E+9 Ω/sq

Show Supplier Material materials with Surface resistivity of 1.00E+9 Ω/sq

ASTM D257

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

24 g/10min

Show Supplier Material materials with Melt mass-flow rate of 24 g/10min

ASTM D1238, 230°C/5kg

Shrinkage

23.0 °C

0.92 %

Show Supplier Material materials with Shrinkage of 0.92 %

ASTM D1238, Mold Shrinkage

Technological properties

Property
Application areas

Hard drive and memory fixtures, Computer work surfaces, ESD circular disc, ESD protection board, ESD electric & housing spare parts, Electric accessories

Certifications

RoHS

Color

Transparent

Processing methods

Injection molding - Drying time: 4hrs, temperature: 80°C - injection temperature: 180-220°C