PC B3400 BK

Alternative and trade names
CON PC B3400 BK
Want to keep this datasheet? Save it now in your required format

Description

Polycarbonate (PC) resin with carbon black added for electrically conductivity.

This material data has been provided by Dongguan SUGO Plastics Technology.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.42 g/cm³

Show Supplier Material materials with Density of 1.42 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

5.1 %

Show Supplier Material materials with Elongation of 5.1 %

ASTM D638

Flexural modulus

23.0 °C

1.71 GPa

Show Supplier Material materials with Flexural modulus of 1.71 GPa

ASTM D790

Flexural strength

23.0 °C

310 MPa

Show Supplier Material materials with Flexural strength of 310 MPa

ASTM D790

Impact strength, Izod notched, ASTM

23.0 °C

18 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 18 J/m

ASTM D256, 3.2mm

Tensile strength

23.0 °C

49 MPa

Show Supplier Material materials with Tensile strength of 49 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

320 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 320 °C

ASTM D648

Flammability

V2 UL94

Electrical

PropertyTemperatureValueComment

Surface resistivity

23.0 °C

1000 - 100000 Ω/sq

Show Supplier Material materials with Surface resistivity of 1000 - 100000 Ω/sq

ASTM D257

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

7.5 g/10min

Show Supplier Material materials with Melt mass-flow rate of 7.5 g/10min

ASTM D1238, 230°C/5kg

Shrinkage

23.0 °C

0.15 - 0.2 %

Show Supplier Material materials with Shrinkage of 0.15 - 0.2 %

ASTM D1238, Mold Shrinkage

Technological properties

Property
Application areas

ESD IC tray, ESD lens tray, Conductive tweenzers, ESD container, ESD electric & housing spare parts, Conductive communication equipment

Certifications

RoHS

Color

Black

Processing methods

Injection molding - Drying time: 4hrs, temperature: 120°C - Mold temperature:100-120°C - injection temperature: 120°C