MPPO F1310 BK TDS

Alternative and trade names
CON MPPO F1310 BK TDS
Want to keep this datasheet? Save it now in your required format

Description

Modified PPO compound filled with carbon fiber for electrical conductivity.

This material data has been provided by Dongguan SUGO Plastics Technology.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.3 g/cm³

Show Supplier Material materials with Density of 1.3 g/cm³

ASTM D792

Water absorption

23.0 °C

3.45 %

Show Supplier Material materials with Water absorption of 3.45 %

ASTM D570, 24hr and 50%RH

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

8 %

Show Supplier Material materials with Elongation of 8 %

ASTM D638

Flexural modulus

23.0 °C

10.63 GPa

Show Supplier Material materials with Flexural modulus of 10.63 GPa

ASTM D790

Flexural strength

23.0 °C

144 MPa

Show Supplier Material materials with Flexural strength of 144 MPa

ASTM D790

Impact strength, Izod notched, ASTM

23.0 °C

2.6 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 2.6 J/m

ASTM D256

Tensile strength

23.0 °C

108 MPa

Show Supplier Material materials with Tensile strength of 108 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

160 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 160 °C

ASTM D648

Electrical

PropertyTemperatureValueComment

Surface resistivity

23.0 °C

10000 - 1000000 Ω/sq

Show Supplier Material materials with Surface resistivity of 10000 - 1000000 Ω/sq

ASTM D257

Rheological Properties

PropertyValueComment

Melt mass-flow rate

3.45 g/10min

Show Supplier Material materials with Melt mass-flow rate of 3.45 g/10min

ASTM D2240, 180°C/5kg

Technological properties

Property
Certifications

RoHS

Color

Black

Fillers

Carbon Fiber

Processing methods

Injection molding - Drying time: 4hrs, temperature: 150°C - mold temperature: 130°C - injection temperature: 280-320°C