General

PropertyTemperatureValueComment

Density

23.0 °C

1.04 g/cm³

Show Supplier Material materials with Density of 1.04 g/cm³

ASTM D792

Water absorption

23.0 °C

0.1 %

Show Supplier Material materials with Water absorption of 0.1 %

maximum, ASTM D570

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

35 %

Show Supplier Material materials with Elongation of 35 %

ASTM D638

Flexural modulus

23.0 °C

2.26 GPa

Show Supplier Material materials with Flexural modulus of 2.26 GPa

ASTM D790

Flexural strength

23.0 °C

58.8 MPa

Show Supplier Material materials with Flexural strength of 58.8 MPa

ASTM D 790

Hardness, Rockwell L

23.0 °C

68 [-]

Show Supplier Material materials with Hardness, Rockwell L of 68 [-]

ASTM D785

Tensile strength

23.0 °C

31.38 MPa

Show Supplier Material materials with Tensile strength of 31.38 MPa

ASTM D638

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

5E-5 - 1E-4 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 5E-5 - 1E-4 1/K

ASTM D696

Heat deflection temperature, 0.45 MPa

85 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 85 °C

ASTM D648

Relative temperature index, electrical

50 °C

Show Supplier Material materials with Relative temperature index, electrical of 50 °C

UL 746B

Relative temperature index, mechanical impact

50 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C

UL 746B

Relative temperature index, mechanical strength

50 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C

UL 746B

Vicat softening temperature

107 °C

Show Supplier Material materials with Vicat softening temperature of 107 °C

ASTM D1525

Flammability

HB UL94

Rheological Properties

PropertyValueComment

Melt mass-flow rate

5 g/10min

Show Supplier Material materials with Melt mass-flow rate of 5 g/10min

ASTM D1238

Technological properties

Property
Application areas

AUDIO/TV/VTR HOUSING, HOUSEHOLD ITEMS