HIPS IT 43

Alternative and trade names
IT 43, PS-I
Want to keep this datasheet? Save it now in your required format

Description

High Impact Polystyrene (HIPS) that indicates good flow.

This material data has been provided by Toling Corporation Sdn Bhd .

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.04 g/cm³

Show Supplier Material materials with Density of 1.04 g/cm³

ASTM D792

Water absorption

23.0 °C

0.1 %

Show Supplier Material materials with Water absorption of 0.1 %

maximum, ASTM D570

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

35 %

Show Supplier Material materials with Elongation of 35 %

ASTM D638

Flexural modulus

23.0 °C

1.91 GPa

Show Supplier Material materials with Flexural modulus of 1.91 GPa

ASTM D790

Flexural strength

23.0 °C

45.1 MPa

Show Supplier Material materials with Flexural strength of 45.1 MPa

ASTM D 790

Hardness, Rockwell L

23.0 °C

50 [-]

Show Supplier Material materials with Hardness, Rockwell L of 50 [-]

ASTM D785

Tensile strength

23.0 °C

24.52 MPa

Show Supplier Material materials with Tensile strength of 24.52 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

83 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 83 °C

ASTM D648

Vicat softening temperature

106 °C

Show Supplier Material materials with Vicat softening temperature of 106 °C

ASTM D1525

Flammability

HB UL94

Rheological Properties

PropertyValueComment

Melt mass-flow rate

8.5 g/10min

Show Supplier Material materials with Melt mass-flow rate of 8.5 g/10min

ASTM D1238

Technological properties

Property
Application areas

Compounding grades