PS 1450

Alternative and trade names
1450
Want to keep this datasheet? Save it now in your required format

Description

TPSC, Polystyrene Crystal 1450 is a high heat resistant, easy flow polystyrene for foam extrusion and injection molding applications. It offers optimum fluidity and excellent thermal properties for foam extrusion and injection molding.

This material data has been provided by Toling Corporation Sdn Bhd .

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.04 g/cm³

Show Supplier Material materials with Density of 1.04 g/cm³

ASTM D792

Water absorption

23.0 °C

0.04 %

Show Supplier Material materials with Water absorption of 0.04 %

ASTM D570

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

2 %

Show Supplier Material materials with Elongation of 2 %

ASTM D638

Flexural modulus

23.0 °C

3.24 GPa

Show Supplier Material materials with Flexural modulus of 3.24 GPa

ASTM D790

Hardness, Rockwell L

23.0 °C

70 [-]

Show Supplier Material materials with Hardness, Rockwell L of 70 [-]

ASTM D785

Impact strength, Izod unnotched

23.0 °C

8 kJ/m²

Show Supplier Material materials with Impact strength, Izod unnotched of 8 kJ/m²

ISO 180

Yield strength

23.0 °C

50 MPa

Show Supplier Material materials with Yield strength of 50 MPa

ASTM D638

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

8.9E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 8.9E-5 1/K

ASTM D696

Heat deflection temperature, 1.80 MPa

85 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 85 °C

ASTM D648

Vicat softening temperature

103 °C

Show Supplier Material materials with Vicat softening temperature of 103 °C

ASTM D1525

Electrical

PropertyTemperatureValueComment

Dielectric strength

23.0 °C

152 kV/mm

Show Supplier Material materials with Dielectric strength of 152 kV/mm

ASTM D149

Surface resistivity

23.0 °C

1.00E+13 Ω/sq

Show Supplier Material materials with Surface resistivity of 1.00E+13 Ω/sq

IEC 93

Rheological Properties

PropertyValueComment

Melt mass-flow rate

5 g/10min

Show Supplier Material materials with Melt mass-flow rate of 5 g/10min

ASTM D1238

Technological properties

Property
Application areas

EXTRUSION SHEET, FOAM EXTRUSION, HOUSEHOLD