General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.27 g/cm³ Show Supplier Material materials with Density of 1.27 g/cm³ | ASTM D792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 180 % Show Supplier Material materials with Elongation of 180 % | ASTM D638 |
Elongation at yield | 23.0 °C | 4.5 % Show Supplier Material materials with Elongation at yield of 4.5 % | ASTM D638 |
Flexural modulus | 23.0 °C | 2.1 GPa Show Supplier Material materials with Flexural modulus of 2.1 GPa | ASTM D790 |
Flexural strength | 23.0 °C | 69 MPa Show Supplier Material materials with Flexural strength of 69 MPa | ASTM D790 |
Hardness, Rockwell R | 23.0 °C | 108 [-] Show Supplier Material materials with Hardness, Rockwell R of 108 [-] | ASTM D785 |
Impact strength, Charpy notched | 23.0 °C | 105 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 105 kJ/m² | ASTM D 256 |
Tensile strength | 23.0 °C | 29 MPa Show Supplier Material materials with Tensile strength of 29 MPa | ASTM D638 |
Yield strength | 23.0 °C | 50 MPa Show Supplier Material materials with Yield strength of 50 MPa | ASTM D638 |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 70 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 70 °C | ASTM D648 | |
Heat deflection temperature, 1.80 MPa | 62 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 62 °C | ASTM D648 | |
Flammability | HB for 1.9mm and V-2 for 0.4mm UL94 |
Optical
Property | Value | Comment |
---|---|---|
Transmission | 90 % Show Supplier Material materials with Transmission of 90 % | ASTM D1003 at 3000 μm |
Technological properties
Property | ||
---|---|---|
Application areas | Sheet, Cosmetic, Construction, Food, Drink, Deco Film |