PETG K 2012

Alternative and trade names
K 2012
Want to keep this datasheet? Save it now in your required format

This material data has been provided by Toling Corporation Sdn Bhd .

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.27 g/cm³

Show Supplier Material materials with Density of 1.27 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

180 %

Show Supplier Material materials with Elongation of 180 %

ASTM D638

Elongation at yield

23.0 °C

4.5 %

Show Supplier Material materials with Elongation at yield of 4.5 %

ASTM D638

Flexural modulus

23.0 °C

2.1 GPa

Show Supplier Material materials with Flexural modulus of 2.1 GPa

ASTM D790

Flexural strength

23.0 °C

69 MPa

Show Supplier Material materials with Flexural strength of 69 MPa

ASTM D790

Hardness, Rockwell R

23.0 °C

108 [-]

Show Supplier Material materials with Hardness, Rockwell R of 108 [-]

ASTM D785

Impact strength, Charpy notched

23.0 °C

105 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 105 kJ/m²

ASTM D 256

Tensile strength

23.0 °C

29 MPa

Show Supplier Material materials with Tensile strength of 29 MPa

ASTM D638

Yield strength

23.0 °C

50 MPa

Show Supplier Material materials with Yield strength of 50 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

70 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 70 °C

ASTM D648

Heat deflection temperature, 1.80 MPa

62 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 62 °C

ASTM D648

Flammability

HB for 1.9mm and V-2 for 0.4mm UL94

Optical

PropertyValueComment

Transmission

90 %

Show Supplier Material materials with Transmission of 90 %

ASTM D1003 at 3000 μm

Technological properties

Property
Application areas

Sheet, Cosmetic, Construction, Food, Drink, Deco Film