General
Property | Value | Temperature |
---|---|---|
Lateral flake size | 80 - 500 nm Show Supplier Material materials with Lateral flake size of 80 - 500 nm | |
Layer thickness | 3E-3 µm Show Supplier Material materials with Layer thickness of 3E-3 µm at 23.0 °C | 23.0 °C |
Viscosity | 3E-3 Pa·s Show Supplier Material materials with Viscosity of 3E-3 Pa·s at 23.0 °C | 23.0 °C |
Electrical
Property | Value | Temperature | Comment |
---|---|---|---|
Surface resistivity | 30 - 4000 Ω/sq Show Supplier Material materials with Surface resistivity of 30 - 4000 Ω/sq at 23.0 °C | 23.0 °C | Minimum for 80nm and Maximum for 2µm thickness |
Technological properties
Property | ||
---|---|---|
Application areas | flexible electronics | |
Processing methods | Ink jet printing, Vacuum Filtration, Meyer Bar Coating - with a drying condition of 100℃ for 10 min |