DIN 1712-3 Grade 3.0205 F

Want to keep this datasheet? Save it now in your required format

Description

Pure aluminium This material is well anodically oxidizable and has a good electrical and thermal conductivity. The splinter-giving workability is bad because of danger of smearing. Its mechanical strength is low, the plasticity high. The forming capacity and the chemical as well as weather proofness are excellent. The materialist it for welding and braze welding well suitably. Application: Apparatus engineering, roll bond, z-bond, household devices, camp and tansport tanks for the chemical, pharmaceutical and food industry, roofings, linings, arts and crafts, packing, flow pressed parts (tubes, tube, doses, bottles), metal goods, motor vehicle characteristics.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

2.71 g/cm³

Show Material materials with Density of 2.71 g/cm³

F

EN 573-3, EN 485, EN 570, EN 755

20.0 °C

2.71 g/cm³

Show Material materials with Density of 2.71 g/cm³

F

DIN 1712-3, EN 573-3, EN 573-4

Profile, Rod, Tube

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

69.0 GPa

Show Material materials with Elastic modulus of 69.0 GPa

F

EN 573-3, EN 485, EN 570, EN 755

20.0 °C

60.0 - 65.0 GPa

Show Material materials with Elastic modulus of 60.0 - 65.0 GPa

F

DIN 1712-3, EN 573-3, EN 573-4

Profile, Rod, Tube

Elongation

18.0 %

Show Material materials with Elongation of 18.0 %

F

EN 573-3, EN 755

A50

20.0 %

Show Material materials with Elongation of 20.0 %

F

EN 573-3, EN 755

A100

20.0 °C

16.0 %

Show Material materials with Elongation of 16.0 %

F

DIN 1712-3, EN 573-3, EN 573-4

Profile, Rod, Tube

A10

20.0 °C

18.0 %

Show Material materials with Elongation of 18.0 %

F

DIN 1712-3, EN 573-3, EN 573-4

Profile, Rod, Tube

Hardness, Brinell

25.0 [-]

Show Material materials with Hardness, Brinell of 25.0 [-]

F

EN 573-3, EN 570

20.0 °C

22.0 [-]

Show Material materials with Hardness, Brinell of 22.0 [-]

F

DIN 1712-3, EN 573-3, EN 573-4

Profile, Rod, Tube

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 1000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 1000 Series Aluminium

Shear modulus

25.9 GPa

Show Material materials with Shear modulus of 25.9 GPa

F

EN 573-3, EN 485, EN 570, EN 755

20.0 °C

24.0 - 26.0 GPa

Show Material materials with Shear modulus of 24.0 - 26.0 GPa

F

DIN 1712-3, EN 573-3, EN 573-4

Profile, Rod, Tube

Tensile strength

75.0 MPa

Show Material materials with Tensile strength of 75.0 MPa

F

EN 573-3, EN 485, EN 755

20.0 °C

75.0 MPa

Show Material materials with Tensile strength of 75.0 MPa

F

DIN 1712-3, EN 573-3, EN 573-4

Profile, Rod, Tube

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

-50 °C

2.17e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.17e-05 1/K

F

EN 573-3, EN 485, EN 570, EN 755, DIN 1712-3, EN 573-4

Profile, Rod, Tube

-50.0 °C

2.17e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.17e-05 1/K

F

EN 573-3, EN 485, EN 570, EN 755, DIN 1712-3, EN 573-4

Profile, Rod, Tube

20 °C

2.17e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.17e-05 1/K

F

EN 573-3, EN 485, EN 570, EN 755, DIN 1712-3, EN 573-4

Profile, Rod, Tube

20 °C

2.35e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K

F

EN 573-3, EN 485, EN 570, EN 755, DIN 1712-3, EN 573-4

Profile, Rod, Tube

20 °C

2.4399999999999997e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.4399999999999997e-05 1/K

F

EN 573-3, EN 485, EN 570, EN 755

20 °C

2.5399999999999997e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.5399999999999997e-05 1/K

F

EN 573-3, EN 485, EN 570, EN 755

100 °C

2.35e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K

F

EN 573-3, EN 485, EN 570, EN 755, DIN 1712-3, EN 573-4

Profile, Rod, Tube

100.0 °C

2.35e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K

F

EN 573-3, EN 485, EN 570, EN 755, DIN 1712-3, EN 573-4

Profile, Rod, Tube

200 °C

2.4399999999999997e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.4399999999999997e-05 1/K

F

EN 573-3, EN 485, EN 570, EN 755

200.0 °C

2.44e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.44e-05 1/K

F

DIN 1712-3, EN 573-3, EN 573-4

Profile, Rod, Tube

300 °C

2.5399999999999997e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.5399999999999997e-05 1/K

F

EN 573-3, EN 485, EN 570, EN 755

300.0 °C

2.54e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.54e-05 1/K

F

DIN 1712-3, EN 573-3, EN 573-4

Profile, Rod, Tube

Melting point

644.0 - 657.0 °C

Show Material materials with Melting point of 644.0 - 657.0 °C

F

EN 573-3, EN 485, EN 570, EN 755

Specific heat capacity

900.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 900.0 - 963.0 J/(kg·K)

Typical for Wrought 1000 Series Aluminium

Thermal conductivity

20.0 °C

205.0 - 210.0 W/(m·K)

Show Material materials with Thermal conductivity of 205.0 - 210.0 W/(m·K)

F

DIN 1712-3, EN 573-3, EN 573-4, EN 485, EN 570, EN 755

Profile, Rod, Tube

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical conductivity

33000000.0 - 34000000.0 S/m

Show Material materials with Electrical conductivity of 33000000.0 - 34000000.0 S/m

F

EN 573-3, EN 485, EN 570, EN 755

20.0 °C

34400000.0 - 35500000.0 S/m

Show Material materials with Electrical conductivity of 34400000.0 - 35500000.0 S/m

F

DIN 1712-3, EN 573-3, EN 573-4

Profile, Rod, Tube

Electrical resistivity

2.94e-08 - 3.03e-08 Ω·m

Show Material materials with Electrical resistivity of 2.94e-08 - 3.03e-08 Ω·m

F

EN 573-3, EN 485, EN 570, EN 755

Chemical properties

PropertyValueConditionRelated StandardsShape

Aluminium

99.0 %

Show Material materials with Aluminium of 99.0 %

F

EN 573-3, EN 485, EN 570, EN 755

Copper

0.05 %

Show Material materials with Copper of 0.05 %

F

DIN 1712-3, EN 573-3, EN 573-4, EN 485, EN 570, EN 755

Profile, Rod, Tube

Magnesium

0.05 %

Show Material materials with Magnesium of 0.05 %

F

DIN 1712-3, EN 573-3, EN 573-4, EN 485, EN 570, EN 755

Profile, Rod, Tube

Manganese

0.05 %

Show Material materials with Manganese of 0.05 %

F

DIN 1712-3, EN 573-3, EN 573-4, EN 485, EN 570, EN 755

Profile, Rod, Tube

Titanium

0.05 %

Show Material materials with Titanium of 0.05 %

F

DIN 1712-3, EN 573-3, EN 573-4, EN 485, EN 570, EN 755

Profile, Rod, Tube

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

F

DIN 1712-3, EN 573-3, EN 573-4, EN 485, EN 570, EN 755

Profile, Rod, Tube

Technological properties

Property
Anodizing

decorative: acceptable, Protective: very good

Brazing

hard brazing (with flux/ without flux): very good / very good, friction soldering: very good, soft brazing with flux: very good

Corrosion properties

Seawater: sufficient, weathering: acceptable

Workability

Bending / Spinning (cold): very good / very good, Impact extrusion (cold): very good, Deep drawing / upsetting (Condition) very good (H12) / very good (H12)