General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Density | 20.0 °C | 2.7 g/cm³ Show Material materials with Density of 2.7 g/cm³ | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | -195.0 °C | 78.4 GPa Show Material materials with Elastic modulus of 78.4 GPa | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip | |
-85.0 °C | 73.5 GPa Show Material materials with Elastic modulus of 73.5 GPa | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip | ||
-30.0 °C | 71.4 GPa Show Material materials with Elastic modulus of 71.4 GPa | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip | ||
20.0 °C | 60.0 - 70.0 GPa Show Material materials with Elastic modulus of 60.0 - 70.0 GPa | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip | ||
20.0 °C | 70.0 GPa Show Material materials with Elastic modulus of 70.0 GPa | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip | ||
100.0 °C | 68.6 GPa Show Material materials with Elastic modulus of 68.6 GPa | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip | ||
150.0 °C | 66.5 GPa Show Material materials with Elastic modulus of 66.5 GPa | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip | ||
200.0 °C | 63.0 GPa Show Material materials with Elastic modulus of 63.0 GPa | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip | ||
250.0 °C | 56.0 GPa Show Material materials with Elastic modulus of 56.0 GPa | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip | ||
Elongation | 20.0 °C | 1.0 % Show Material materials with Elongation of 1.0 % | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Flat | A100 |
20.0 °C | 2.0 % Show Material materials with Elongation of 2.0 % | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip | A10 | |
20.0 °C | 3.0 % Show Material materials with Elongation of 3.0 % | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Strip | ||
Hardness, Brinell | 20.0 °C | 45.0 [-] Show Material materials with Hardness, Brinell of 45.0 [-] | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Strip | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | ||||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | ||||
Shear modulus | 20.0 °C | 25.0 - 26.5 GPa Show Material materials with Shear modulus of 25.0 - 26.5 GPa | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip | |
Tensile strength | 20.0 °C | 150.0 MPa Show Material materials with Tensile strength of 150.0 MPa | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Strip | |
20.0 °C | 150.0 - 190.0 MPa Show Material materials with Tensile strength of 150.0 - 190.0 MPa | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Flat |
Thermal
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | -50.0 °C | 2.17e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.17e-05 1/K | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip | |
100.0 °C | 2.35e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip | ||
200.0 °C | 2.44e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.44e-05 1/K | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip | ||
300.0 °C | 2.54e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.54e-05 1/K | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip | ||
Melting point | 645.0 - 660.0 °C Show Material materials with Melting point of 645.0 - 660.0 °C | Typical for Wrought 1000 Series Aluminium | ||||
Specific heat capacity | 20.0 °C | 900.0 J/(kg·K) Show Material materials with Specific heat capacity of 900.0 J/(kg·K) | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip | |
Thermal conductivity | 20.0 °C | 210.0 - 220.0 W/(m·K) Show Material materials with Thermal conductivity of 210.0 - 220.0 W/(m·K) | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Electrical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Electrical conductivity | 20.0 °C | 34800000.0 - 36000000.0 S/m Show Material materials with Electrical conductivity of 34800000.0 - 36000000.0 S/m | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip | |
Electrical resistivity | 2.7e-08 - 3e-08 Ω·m Show Material materials with Electrical resistivity of 2.7e-08 - 3e-08 Ω·m | Typical for Wrought 1000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Copper | 0.05 Show Material materials with Copper of 0.05 | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Iron | 0.4 Show Material materials with Iron of 0.4 | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Magnesium | 0.05 Show Material materials with Magnesium of 0.05 | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Manganese | 0.05 Show Material materials with Manganese of 0.05 | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Silicon | 0.25 Show Material materials with Silicon of 0.25 | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Titanium | 0.05 Show Material materials with Titanium of 0.05 | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Zinc | 0.07 Show Material materials with Zinc of 0.07 | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent | |
Workability | Excellent workability. |