Description

The alloy AlMn1Mg0,5 is similarly to AlMn1 in its properties. It reaches strength up to F 25. The alloy belongs to the nature-hard aluminum materials. A strength increase can only occure by cold forming. It is very well hot and cold formable and is suitable to the deep-drawing (no lappet formation). The alloy AlMn1Mg0,5 is very well corrosion resistant and is sea water steady. As semi-finished material it is present in accordance with DIN 1788 and DIN 1745 only as sheet metal or strip. Application: Mainly in the packing for cans (lower parts), for menu bowls, for covers. In the building industry for claddings, roofings, for sun protection facilities (roller schutter, lamella net curtain) and for roll gates as well as for flexible pipes and in the construction of vehicles.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

2.72 g/cm³

Show Material materials with Density of 2.72 g/cm³

H24

EN 573-3, EN 1592, EN 485, EN 546

20.0 °C

2.72 g/cm³

Show Material materials with Density of 2.72 g/cm³

H24

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Flat, Strip

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Bending angle 180°

1.5 °/t

Show Material materials with Bending angle 180° of 1.5 °/t

H24

EN 573-3, EN 485

Bending angle 90°

0.5 °/t

Show Material materials with Bending angle 90° of 0.5 °/t

H24

EN 573-3, EN 485

1.0 °/t

Show Material materials with Bending angle 90° of 1.0 °/t

H24

EN 573-3, EN 485

1.5 °/t

Show Material materials with Bending angle 90° of 1.5 °/t

H24

EN 573-3, EN 485

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

H24

EN 573-3, EN 1592, EN 485, EN 546

20.0 °C

65.0 GPa

Show Material materials with Elastic modulus of 65.0 GPa

H24

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Flat, Strip

Elongation

3.0 %

Show Material materials with Elongation of 3.0 %

H24

EN 573-3, EN 546

A50

4.0 %

Show Material materials with Elongation of 4.0 %

H24

EN 573-3, EN 485, EN 546

A50

7.0 %

Show Material materials with Elongation of 7.0 %

H24

EN 573-3, EN 1592

A100

20.0 °C

5.0 %

Show Material materials with Elongation of 5.0 %

H24

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

A10

20.0 °C

5.0 %

Show Material materials with Elongation of 5.0 %

H24

DIN 1725-1, EN 573-3, EN 573-4

Flat

A100

20.0 °C

6.0 %

Show Material materials with Elongation of 6.0 %

H24

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Hardness, Brinell

52.0 [-]

Show Material materials with Hardness, Brinell of 52.0 [-]

H24

EN 573-3, EN 485

20.0 °C

55.0 [-]

Show Material materials with Hardness, Brinell of 55.0 [-]

H24

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 3000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 3000 Series Aluminium

Shear modulus

20.0 °C

26.5

Show Material materials with Shear modulus of 26.5

H24

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Flat, Strip

Tensile strength

170.0 - 215.0 MPa

Show Material materials with Tensile strength of 170.0 - 215.0 MPa

H24

EN 573-3, EN 485

180.0 - 225.0 MPa

Show Material materials with Tensile strength of 180.0 - 225.0 MPa

H24

EN 573-3, EN 546

200.0 MPa

Show Material materials with Tensile strength of 200.0 MPa

H24

EN 573-3, EN 1592

20.0 °C

175.0 - 215.0 MPa

Show Material materials with Tensile strength of 175.0 - 215.0 MPa

H24

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

20.0 °C

185.0 - 225.0 MPa

Show Material materials with Tensile strength of 185.0 - 225.0 MPa

H24

DIN 1725-1, EN 573-3, EN 573-4

Flat

Thermal

PropertyTemperatureValueConditionRelated StandardsShape

Coefficient of thermal expansion

20 °C

2.3199999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3199999999999998e-05 1/K

H24

EN 573-3, EN 1592, EN 485, EN 546

100 °C

2.3199999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3199999999999998e-05 1/K

H24

EN 573-3, EN 1592, EN 485, EN 546

Melting point

630.0 - 654.0 °C

Show Material materials with Melting point of 630.0 - 654.0 °C

H24

EN 573-3, EN 1592, EN 485, EN 546

Specific heat capacity

20.0 °C

893.0 J/(kg·K)

Show Material materials with Specific heat capacity of 893.0 J/(kg·K)

H24

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Flat, Strip

Thermal conductivity

160.0 - 190.0 W/(m·K)

Show Material materials with Thermal conductivity of 160.0 - 190.0 W/(m·K)

H24

EN 573-3, EN 1592, EN 485, EN 546

20.0 °C

200.0 W/(m·K)

Show Material materials with Thermal conductivity of 200.0 W/(m·K)

H24

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Flat, Strip

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical conductivity

23000000.0 - 25000000.0 S/m

Show Material materials with Electrical conductivity of 23000000.0 - 25000000.0 S/m

H24

EN 573-3, EN 1592, EN 485, EN 546

20.0 °C

28000000.0 S/m

Show Material materials with Electrical conductivity of 28000000.0 S/m

H24

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Flat, Strip

Electrical resistivity

4e-08 - 4.35e-08 Ω·m

Show Material materials with Electrical resistivity of 4e-08 - 4.35e-08 Ω·m

H24

EN 573-3, EN 1592, EN 485, EN 546

Chemical properties

PropertyValueConditionRelated StandardsShape

Chromium

0.1 %

Show Material materials with Chromium of 0.1 %

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 1592, EN 485, EN 546

Sheet, Flat, Strip

Copper

0.3 %

Show Material materials with Copper of 0.3 %

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 1592, EN 485, EN 546

Sheet, Flat, Strip

Iron

0.7 %

Show Material materials with Iron of 0.7 %

H24

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Flat, Strip

0.70 %

Show Material materials with Iron of 0.70 %

H24

EN 573-3, EN 1592, EN 485, EN 546

Magnesium

0.2 - 0.6 %

Show Material materials with Magnesium of 0.2 - 0.6 %

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 1592, EN 485, EN 546

Sheet, Flat, Strip

Manganese

1.0 - 1.5 %

Show Material materials with Manganese of 1.0 - 1.5 %

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 1592, EN 485, EN 546

Sheet, Flat, Strip

Silicon

0.6 %

Show Material materials with Silicon of 0.6 %

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 1592, EN 485, EN 546

Sheet, Flat, Strip

Titanium

0.1 %

Show Material materials with Titanium of 0.1 %

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 1592, EN 485, EN 546

Sheet, Flat, Strip

Zinc

0.25 %

Show Material materials with Zinc of 0.25 %

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 1592, EN 485, EN 546

Sheet, Flat, Strip

Technological properties

Property
Anodizing

decorative: sufficient, Protective: very good

Corrosion properties

Seawater: very good, weathering: very good

Workability

Bending / Spinning (cold): good / acceptable, Impact extrusion (cold): acceptable, Deep drawing / upsetting (Condition) very good (O) / acceptable (H12)