Description

The alloy AlFeSi is alloyed for increasing the strength increase with Fe and Si. The material belongs to the nature-hard aluminum materials. A strength increase can be achieved only by cold forming. The alloy AlFeSi is very well cold and warm formable and has a good thermal and relatively good electrical conductivity. The material is particularly suitable for deep-drawing. It is well solderable. The material is to be oxidized well anodically, i.e. a shining clean surface develops. It is standardised as sheet metal or strip (DIN 1788 and DIN 1745). Application: for screw-type caps, for menu bowls, for light containers, bottle caps, cover containers and other form packing, for metal goods, like trim, decorated tiles, flexible pipes, various deep-drawing products, for heat exchangers and radiator fins

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

2.71 g/cm³

Show Material materials with Density of 2.71 g/cm³

H24

EN 573-3, EN 485, EN 541, EN 546, EN 683

20.0 °C

2.71 g/cm³

Show Material materials with Density of 2.71 g/cm³

H24

DIN 1725-1, EN 573-3, EN 573-4

Flat

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

H24

EN 573-3, EN 485, EN 541, EN 546, EN 683

Elongation

2.0 %

Show Material materials with Elongation of 2.0 %

H24

EN 573-3, EN 541, EN 546

A50

3.0 %

Show Material materials with Elongation of 3.0 %

H24

EN 573-3, EN 485, EN 546

A50

4.0 %

Show Material materials with Elongation of 4.0 %

H24

EN 573-3, EN 485, EN 546, EN 683

A50

5.0 %

Show Material materials with Elongation of 5.0 %

H24

EN 573-3, EN 485, EN 546, EN 683

A50

6.0 %

Show Material materials with Elongation of 6.0 %

H24

EN 573-3, EN 485, EN 683

A50

7.0 %

Show Material materials with Elongation of 7.0 %

H24

EN 573-3, EN 485

A50

20.0 °C

4.0 %

Show Material materials with Elongation of 4.0 %

H24

DIN 1725-1, EN 573-3, EN 573-4

Flat

A10

20.0 °C

5.0 %

Show Material materials with Elongation of 5.0 %

H24

DIN 1725-1, EN 573-3, EN 573-4

Flat

A10

20.0 °C

7.0 %

Show Material materials with Elongation of 7.0 %

H24

DIN 1725-1, EN 573-3, EN 573-4

Flat

Hardness, Brinell

40.0 [-]

Show Material materials with Hardness, Brinell of 40.0 [-]

H24

EN 573-3, EN 485

20.0 °C

40.0 [-]

Show Material materials with Hardness, Brinell of 40.0 [-]

H24

DIN 1725-1, EN 573-3, EN 573-4

Flat

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 8000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 8000 Series Aluminium

Tensile strength

110.0 - 165.0 MPa

Show Material materials with Tensile strength of 110.0 - 165.0 MPa

H24

EN 573-3, EN 546, EN 683

120.0 - 160.0 MPa

Show Material materials with Tensile strength of 120.0 - 160.0 MPa

H24

EN 573-3, EN 541

125.0 - 165.0 MPa

Show Material materials with Tensile strength of 125.0 - 165.0 MPa

H24

EN 573-3, EN 485

20.0 °C

130.0 - 170.0 MPa

Show Material materials with Tensile strength of 130.0 - 170.0 MPa

H24

DIN 1725-1, EN 573-3, EN 573-4

Flat

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

20 °C

2.35e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K

H24

EN 573-3, EN 485, EN 541, EN 546, EN 683

100 °C

2.35e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K

H24

EN 573-3, EN 485, EN 541, EN 546, EN 683

Melting point

640.0 - 655.0 °C

Show Material materials with Melting point of 640.0 - 655.0 °C

H24

EN 573-3, EN 485, EN 541, EN 546, EN 683

Specific heat capacity

920.0 J/(kg·K)

Show Material materials with Specific heat capacity of 920.0 J/(kg·K)

Typical for Wrought 8000 Series Aluminium

Thermal conductivity

20.0 °C

210.0 - 220.0 W/(m·K)

Show Material materials with Thermal conductivity of 210.0 - 220.0 W/(m·K)

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683

Flat

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical conductivity

20.0 °C

34000000.0 - 35000000.0 S/m

Show Material materials with Electrical conductivity of 34000000.0 - 35000000.0 S/m

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683

Flat

Electrical resistivity

2.86e-08 - 2.94e-08 Ω·m

Show Material materials with Electrical resistivity of 2.86e-08 - 2.94e-08 Ω·m

H24

EN 573-3, EN 485, EN 541, EN 546, EN 683

Chemical properties

PropertyValueConditionRelated StandardsShape

Chromium

0.1 %

Show Material materials with Chromium of 0.1 %

H24

EN 573-3, EN 485, EN 541, EN 546, EN 683

Copper

0.1 %

Show Material materials with Copper of 0.1 %

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683

Flat

Iron

0.5 - 1.0 %

Show Material materials with Iron of 0.5 - 1.0 %

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683

Flat

Magnesium

0.1 %

Show Material materials with Magnesium of 0.1 %

H24

EN 573-3, EN 485, EN 541, EN 546, EN 683

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683

Flat

Silicon

0.4 - 0.8 %

Show Material materials with Silicon of 0.4 - 0.8 %

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683

Flat

Titanium

0.05

Show Material materials with Titanium of 0.05

H24

DIN 1725-1, EN 573-3, EN 573-4

Flat

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

H24

DIN 1725-1, EN 573-3, EN 573-4, EN 485, EN 541, EN 546, EN 683

Flat