General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Density | 20.0 °C | 2.7 g/cm³ Show Material materials with Density of 2.7 g/cm³ | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip, Wire |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 20.0 °C | 70.0 Show Material materials with Elastic modulus of 70.0 | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip, Wire | |
Elongation | 20.0 °C | 14.0 % Show Material materials with Elongation of 14.0 % | O | DIN 1725-1, EN 573-3, EN 573-4 | Wire | A100 |
20.0 °C | 20.0 % Show Material materials with Elongation of 20.0 % | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip, Wire | A10 | |
20.0 °C | 23.0 % Show Material materials with Elongation of 23.0 % | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip | ||
Hardness, Brinell | 20.0 °C | 23.0 [-] Show Material materials with Hardness, Brinell of 23.0 [-] | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip, Wire | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Shear modulus | 20.0 °C | 27.0 Show Material materials with Shear modulus of 27.0 | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip, Wire | |
Tensile strength | 20.0 °C | 70.0 MPa Show Material materials with Tensile strength of 70.0 MPa | O | DIN 1725-1, EN 573-3, EN 573-4 | Wire | |
20.0 °C | 80.0 - 120.0 MPa Show Material materials with Tensile strength of 80.0 - 120.0 MPa | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip |
Thermal
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 2.2e-05 - 2.5e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.2e-05 - 2.5e-05 1/K | Typical for Wrought 5000 Series Aluminium | ||||
Max service temperature | 150.0 °C Show Material materials with Max service temperature of 150.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Melting point | 560.0 - 655.0 °C Show Material materials with Melting point of 560.0 - 655.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Specific heat capacity | 879.0 - 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 879.0 - 963.0 J/(kg·K) | Typical for Wrought 5000 Series Aluminium | ||||
Thermal conductivity | 20.0 °C | 215.0 W/(m·K) Show Material materials with Thermal conductivity of 215.0 W/(m·K) | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip, Wire |
Electrical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Electrical conductivity | 20.0 °C | 35000000.0 Show Material materials with Electrical conductivity of 35000000.0 | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip, Wire | |
Electrical resistivity | 3.3e-08 - 5e-08 Ω·m Show Material materials with Electrical resistivity of 3.3e-08 - 5e-08 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Iron | 0.08 Show Material materials with Iron of 0.08 | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip, Wire |
Magnesium | 0.3 - 0.6 % Show Material materials with Magnesium of 0.3 - 0.6 % | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip, Wire |
Manganese | 0.03 Show Material materials with Manganese of 0.03 | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip, Wire |
Silicon | 0.08 Show Material materials with Silicon of 0.08 | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip, Wire |
Titanium | 0.02 Show Material materials with Titanium of 0.02 | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip, Wire |
Zinc | 0.05 Show Material materials with Zinc of 0.05 | O | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip, Wire |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |