The AlMg alloy is characterised all by a good corrosion resistance. It is sea water steady and resistant to saline atmosphere. The Mg content increase the strength, the cold forming capacity decreases with it. The alloys of this type are nature hard, i.e. only by a cold forming and not by a purposeful heat treatment a strength increase can be attained. The material is well polishabel and anodisable. The splinter-giving machinability becomes better with increasing Mg content just like the weldability. The alloy AlMg1 reaches strength grades to F 22. Application: Their main field of application is the building industry. In the building industry for claddings, roofing and trim, for transport containers. For metal goods, like building fittings, table-ware, flow pressed parts, reflectors. In food industry, for furniture (incl. camping furniture) as well as for describe and for covers with composite slabs (intermediate layer: Polyethylene).

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

20.0 °C

2.69 g/cm³

Show Material materials with Density of 2.69 g/cm³

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

20.0 °C

60.0 - 65.0 GPa

Show Material materials with Elastic modulus of 60.0 - 65.0 GPa

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Elongation

20.0 °C

4.0 %

Show Material materials with Elongation of 4.0 %

T6

DIN 1725-1, EN 573-3, EN 573-4

Strip

A10

20.0 °C

5.0 %

Show Material materials with Elongation of 5.0 %

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

A10

20.0 °C

5.0 %

Show Material materials with Elongation of 5.0 %

T6

DIN 1725-1, EN 573-3, EN 573-4

Strip

20.0 °C

6.0 %

Show Material materials with Elongation of 6.0 %

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Hardness, Brinell

20.0 °C

52.0 [-]

Show Material materials with Hardness, Brinell of 52.0 [-]

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

20.0 °C

57.0 [-]

Show Material materials with Hardness, Brinell of 57.0 [-]

T6

DIN 1725-1, EN 573-3, EN 573-4

Strip

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 5000 Series Aluminium

Shear modulus

20.0 °C

25.0 GPa

Show Material materials with Shear modulus of 25.0 GPa

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Tensile strength

20.0 °C

165.0 - 205.0 MPa

Show Material materials with Tensile strength of 165.0 - 205.0 MPa

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

20.0 °C

190.0 MPa

Show Material materials with Tensile strength of 190.0 MPa

T6

DIN 1725-1, EN 573-3, EN 573-4

Strip

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

-50.0 °C

2.18e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.18e-05 1/K

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

100.0 °C

2.36e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.36e-05 1/K

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

200.0 °C

2.45e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.45e-05 1/K

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

300.0 °C

2.55e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.55e-05 1/K

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Max service temperature

150.0 °C

Show Material materials with Max service temperature of 150.0 °C

Typical for Wrought 5000 Series Aluminium

Melting point

560.0 - 655.0 °C

Show Material materials with Melting point of 560.0 - 655.0 °C

Typical for Wrought 5000 Series Aluminium

Specific heat capacity

20.0 °C

879.0 J/(kg·K)

Show Material materials with Specific heat capacity of 879.0 J/(kg·K)

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Thermal conductivity

20.0 °C

160.0 - 220.0 W/(m·K)

Show Material materials with Thermal conductivity of 160.0 - 220.0 W/(m·K)

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Electrical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Electrical conductivity

20.0 °C

23000000.0 - 31000000.0 S/m

Show Material materials with Electrical conductivity of 23000000.0 - 31000000.0 S/m

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Electrical resistivity

3.3e-08 - 5e-08 Ω·m

Show Material materials with Electrical resistivity of 3.3e-08 - 5e-08 Ω·m

Typical for Wrought 5000 Series Aluminium

Chemical properties

PropertyValueConditionRelated StandardsShape

Chromium

0.1

Show Material materials with Chromium of 0.1

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Copper

0.05

Show Material materials with Copper of 0.05

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Iron

0.45

Show Material materials with Iron of 0.45

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Magnesium

0.7 - 1.1 %

Show Material materials with Magnesium of 0.7 - 1.1 %

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Manganese

0.15

Show Material materials with Manganese of 0.15

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Silicon

0.3

Show Material materials with Silicon of 0.3

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Zinc

0.2

Show Material materials with Zinc of 0.2

T6

DIN 1725-1, EN 573-3, EN 573-4

Sheet, Strip

Technological properties

Property
Workability

Good workability.