The alloys are characterised by a good corrosion resistance. It is sea water steady and resistant to saline atmosphere. The Mg content increases the strength, but the cold forming capacity decreases. The material is nature hard, i.e. only by a cold forming and not by a purposeful heat treatment a strength increase can be attained. It is well polishable and anodisable. The splinter-giving machinability becomes better with increasing Mg content, just as the weldability. From the AlMg alloys the mark AlMg1,5 has to exhibit only relatively small mechanical properties. Standardised semi-finished material only for sheet metal and strips with thickness: > 0.35 mm in accordance to DIN 1745. Application: The main application lies in the building industry. In the building industry for lamella net curtains, rolling shutter, roll gates, in food industry (including table-ware) and for transport containers.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

2.68 g/cm³

Show Material materials with Density of 2.68 g/cm³

H16

EN 573-3, EN 485

2.69 g/cm³

Show Material materials with Density of 2.69 g/cm³

H16

EN 573-3, EN 485

20.0 °C

2.69 g/cm³

Show Material materials with Density of 2.69 g/cm³

H16

DIN 1725-1, EN 573-3, EN 573-4

Flat

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Bending angle 90°

1.0 °/t

Show Material materials with Bending angle 90° of 1.0 °/t

H16

EN 573-3, EN 485

1.5 °/t

Show Material materials with Bending angle 90° of 1.5 °/t

H16

EN 573-3, EN 485

2.5 °/t

Show Material materials with Bending angle 90° of 2.5 °/t

H16

EN 573-3, EN 485

3.0 °/t

Show Material materials with Bending angle 90° of 3.0 °/t

H16

EN 573-3, EN 485

Elastic modulus

69.0 GPa

Show Material materials with Elastic modulus of 69.0 GPa

H16

EN 573-3, EN 485

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

H16

EN 573-3, EN 485

20.0 °C

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

H16

DIN 1725-1, EN 573-3, EN 573-4

Flat

Elongation

1.0 %

Show Material materials with Elongation of 1.0 %

H16

EN 573-3, EN 485

A50

2.0 %

Show Material materials with Elongation of 2.0 %

H16

EN 573-3, EN 485

A50

3.0 %

Show Material materials with Elongation of 3.0 %

H16

EN 573-3, EN 485

A50

20.0 °C

3.0 %

Show Material materials with Elongation of 3.0 %

H16

DIN 1725-1, EN 573-3, EN 573-4

Flat

A10

20.0 °C

4.0 %

Show Material materials with Elongation of 4.0 %

H16

DIN 1725-1, EN 573-3, EN 573-4

Flat

Hardness, Brinell

61.0 [-]

Show Material materials with Hardness, Brinell of 61.0 [-]

H16

EN 573-3, EN 485

20.0 °C

60.0 [-]

Show Material materials with Hardness, Brinell of 60.0 [-]

H16

DIN 1725-1, EN 573-3, EN 573-4

Flat

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 5000 Series Aluminium

Shear modulus

20.0 °C

26.5

Show Material materials with Shear modulus of 26.5

H16

DIN 1725-1, EN 573-3, EN 573-4

Flat

Tensile strength

195.0 - 235.0 MPa

Show Material materials with Tensile strength of 195.0 - 235.0 MPa

H16

EN 573-3, EN 485

20.0 °C

200.0 - 240.0 MPa

Show Material materials with Tensile strength of 200.0 - 240.0 MPa

H16

DIN 1725-1, EN 573-3, EN 573-4

Flat

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

20 °C

2.38e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.38e-05 1/K

H16

EN 573-3, EN 485

100 °C

2.38e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.38e-05 1/K

H16

EN 573-3, EN 485

Max service temperature

150.0 °C

Show Material materials with Max service temperature of 150.0 °C

Typical for Wrought 5000 Series Aluminium

Melting point

620.0 - 650.0 °C

Show Material materials with Melting point of 620.0 - 650.0 °C

H16

EN 573-3, EN 485

625.0 - 650.0 °C

Show Material materials with Melting point of 625.0 - 650.0 °C

H16

EN 573-3, EN 485

Specific heat capacity

879.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 879.0 - 963.0 J/(kg·K)

Typical for Wrought 5000 Series Aluminium

Thermal conductivity

170.0 - 190.0 W/(m·K)

Show Material materials with Thermal conductivity of 170.0 - 190.0 W/(m·K)

H16

EN 573-3, EN 485

193 W/(m·K)

Show Material materials with Thermal conductivity of 193 W/(m·K)

H16

EN 573-3, EN 485

20.0 °C

160.0 - 200.0 W/(m·K)

Show Material materials with Thermal conductivity of 160.0 - 200.0 W/(m·K)

H16

DIN 1725-1, EN 573-3, EN 573-4

Flat

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical conductivity

23000000.0 - 26000000.0 S/m

Show Material materials with Electrical conductivity of 23000000.0 - 26000000.0 S/m

H16

EN 573-3, EN 485

29000000.0 S/m

Show Material materials with Electrical conductivity of 29000000.0 S/m

H16

EN 573-3, EN 485

20.0 °C

28000000.0 - 30000000.0 S/m

Show Material materials with Electrical conductivity of 28000000.0 - 30000000.0 S/m

H16

DIN 1725-1, EN 573-3, EN 573-4

Flat

Electrical resistivity

3.45e-08 Ω·m

Show Material materials with Electrical resistivity of 3.45e-08 Ω·m

H16

EN 573-3, EN 485

3.85e-08 - 4.35e-08 Ω·m

Show Material materials with Electrical resistivity of 3.85e-08 - 4.35e-08 Ω·m

H16

EN 573-3, EN 485

Chemical properties

PropertyValueConditionRelated StandardsShape

Chromium

0.1 %

Show Material materials with Chromium of 0.1 %

H16

DIN 1725-1, EN 573-3, EN 573-4, EN 485

Flat

Copper

0.05 %

Show Material materials with Copper of 0.05 %

H16

DIN 1725-1, EN 573-3, EN 573-4, EN 485

Flat

Iron

0.45 %

Show Material materials with Iron of 0.45 %

H16

DIN 1725-1, EN 573-3, EN 573-4

Flat

0.45 %

Show Material materials with Iron of 0.45 %

H16

EN 573-3, EN 485

Magnesium

1.1 - 1.7 %

Show Material materials with Magnesium of 1.1 - 1.7 %

H16

DIN 1725-1, EN 573-3, EN 573-4, EN 485

Flat

Manganese

0.15 %

Show Material materials with Manganese of 0.15 %

H16

DIN 1725-1, EN 573-3, EN 573-4, EN 485

Flat

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %

H16

DIN 1725-1, EN 573-3, EN 573-4, EN 485

Flat

Zinc

0.2 %

Show Material materials with Zinc of 0.2 %

H16

DIN 1725-1, EN 573-3, EN 573-4, EN 485

Flat

Technological properties

Property
Workability

Good workability.