General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Density | 2.68 g/cm³ Show Material materials with Density of 2.68 g/cm³ | H28 | EN 573-3, EN 485 | ||
2.69 g/cm³ Show Material materials with Density of 2.69 g/cm³ | H28 | EN 573-3, EN 485 | |||
20.0 °C | 2.69 g/cm³ Show Material materials with Density of 2.69 g/cm³ | H28 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Bending angle 90° | 1.5 °/t Show Material materials with Bending angle 90° of 1.5 °/t | H28 | EN 573-3, EN 485 | |||
2.5 °/t Show Material materials with Bending angle 90° of 2.5 °/t | H28 | EN 573-3, EN 485 | ||||
Elastic modulus | 69.0 GPa Show Material materials with Elastic modulus of 69.0 GPa | H28 | EN 573-3, EN 485 | |||
70.0 GPa Show Material materials with Elastic modulus of 70.0 GPa | H28 | EN 573-3, EN 485 | ||||
20.0 °C | 70.0 GPa Show Material materials with Elastic modulus of 70.0 GPa | H28 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | ||
Elongation | 1.0 % Show Material materials with Elongation of 1.0 % | H28 | EN 573-3, EN 485 | A50 | ||
2.0 % Show Material materials with Elongation of 2.0 % | H28 | EN 573-3, EN 485 | A50 | |||
3.0 % Show Material materials with Elongation of 3.0 % | H28 | EN 573-3, EN 485 | A50 | |||
20.0 °C | 5.0 % Show Material materials with Elongation of 5.0 % | H28 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | A10 | |
20.0 °C | 6.0 % Show Material materials with Elongation of 6.0 % | H28 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | ||
Hardness, Brinell | 67.0 [-] Show Material materials with Hardness, Brinell of 67.0 [-] | H28 | EN 573-3, EN 485 | |||
20.0 °C | 65.0 [-] Show Material materials with Hardness, Brinell of 65.0 [-] | H28 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Shear modulus | 20.0 °C | 26.5 Show Material materials with Shear modulus of 26.5 | H28 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | |
Tensile strength | 220.0 MPa Show Material materials with Tensile strength of 220.0 MPa | H28 | EN 573-3, EN 485 | |||
20.0 °C | 225.0 MPa Show Material materials with Tensile strength of 225.0 MPa | H28 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Thermal
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 20 °C | 2.38e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.38e-05 1/K | H28 | EN 573-3, EN 485 | ||
100 °C | 2.38e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.38e-05 1/K | H28 | EN 573-3, EN 485 | |||
Max service temperature | 150.0 °C Show Material materials with Max service temperature of 150.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Melting point | 620.0 - 650.0 °C Show Material materials with Melting point of 620.0 - 650.0 °C | H28 | EN 573-3, EN 485 | |||
625.0 - 650.0 °C Show Material materials with Melting point of 625.0 - 650.0 °C | H28 | EN 573-3, EN 485 | ||||
Specific heat capacity | 879.0 - 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 879.0 - 963.0 J/(kg·K) | Typical for Wrought 5000 Series Aluminium | ||||
Thermal conductivity | 170.0 - 190.0 W/(m·K) Show Material materials with Thermal conductivity of 170.0 - 190.0 W/(m·K) | H28 | EN 573-3, EN 485 | |||
193 W/(m·K) Show Material materials with Thermal conductivity of 193 W/(m·K) | H28 | EN 573-3, EN 485 | ||||
20.0 °C | 160.0 - 200.0 W/(m·K) Show Material materials with Thermal conductivity of 160.0 - 200.0 W/(m·K) | H28 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Electrical
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Electrical conductivity | 23000000.0 - 26000000.0 S/m Show Material materials with Electrical conductivity of 23000000.0 - 26000000.0 S/m | H28 | EN 573-3, EN 485 | ||
29000000.0 S/m Show Material materials with Electrical conductivity of 29000000.0 S/m | H28 | EN 573-3, EN 485 | |||
20.0 °C | 28000000.0 - 30000000.0 S/m Show Material materials with Electrical conductivity of 28000000.0 - 30000000.0 S/m | H28 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | |
Electrical resistivity | 3.45e-08 Ω·m Show Material materials with Electrical resistivity of 3.45e-08 Ω·m | H28 | EN 573-3, EN 485 | ||
3.85e-08 - 4.35e-08 Ω·m Show Material materials with Electrical resistivity of 3.85e-08 - 4.35e-08 Ω·m | H28 | EN 573-3, EN 485 |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chromium | 0.1 % Show Material materials with Chromium of 0.1 % | H28 | DIN 1725-1, EN 573-3, EN 573-4, EN 485 | Flat |
Copper | 0.05 % Show Material materials with Copper of 0.05 % | H28 | DIN 1725-1, EN 573-3, EN 573-4, EN 485 | Flat |
Iron | 0.45 % Show Material materials with Iron of 0.45 % | H28 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
0.45 % Show Material materials with Iron of 0.45 % | H28 | EN 573-3, EN 485 | ||
Magnesium | 1.1 - 1.7 % Show Material materials with Magnesium of 1.1 - 1.7 % | H28 | DIN 1725-1, EN 573-3, EN 573-4, EN 485 | Flat |
Manganese | 0.15 % Show Material materials with Manganese of 0.15 % | H28 | DIN 1725-1, EN 573-3, EN 573-4, EN 485 | Flat |
Silicon | 0.4 % Show Material materials with Silicon of 0.4 % | H28 | DIN 1725-1, EN 573-3, EN 573-4, EN 485 | Flat |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % | H28 | DIN 1725-1, EN 573-3, EN 573-4, EN 485 | Flat |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |