General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Density | 20.0 °C | 2.68 g/cm³ Show Material materials with Density of 2.68 g/cm³ | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip, Wire |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 20.0 °C | 72.0 Show Material materials with Elastic modulus of 72.0 | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip, Wire | |
Elongation | 20.0 °C | 5.0 % Show Material materials with Elongation of 5.0 % | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Wire | A100 |
20.0 °C | 6.0 % Show Material materials with Elongation of 6.0 % | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip | A10 | |
20.0 °C | 7.0 % Show Material materials with Elongation of 7.0 % | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip | ||
20.0 °C | 9.0 % Show Material materials with Elongation of 9.0 % | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Wire | A10 | |
Hardness, Brinell | 20.0 °C | 65.0 [-] Show Material materials with Hardness, Brinell of 65.0 [-] | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Wire | |
20.0 °C | 80.0 [-] Show Material materials with Hardness, Brinell of 80.0 [-] | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Shear modulus | 20.0 °C | 27.0 Show Material materials with Shear modulus of 27.0 | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip, Wire | |
Shear strength | 20.0 °C | 125.0 MPa Show Material materials with Shear strength of 125.0 MPa | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Wire | |
Tensile strength | 20.0 °C | 240.0 MPa Show Material materials with Tensile strength of 240.0 MPa | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Wire | |
20.0 °C | 250.0 - 290.0 MPa Show Material materials with Tensile strength of 250.0 - 290.0 MPa | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip |
Thermal
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | -50.0 °C | 2.21e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.21e-05 1/K | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip, Wire | |
100.0 °C | 2.38e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.38e-05 1/K | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip, Wire | ||
200.0 °C | 2.48e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.48e-05 1/K | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip, Wire | ||
300.0 °C | 2.57e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.57e-05 1/K | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip, Wire | ||
Max service temperature | 150.0 °C Show Material materials with Max service temperature of 150.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Melting point | 560.0 - 655.0 °C Show Material materials with Melting point of 560.0 - 655.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Specific heat capacity | 20.0 °C | 900.0 J/(kg·K) Show Material materials with Specific heat capacity of 900.0 J/(kg·K) | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip, Wire | |
Thermal conductivity | 20.0 °C | 150.0 Show Material materials with Thermal conductivity of 150.0 | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip, Wire |
Electrical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Electrical conductivity | 20.0 °C | 21000000.0 Show Material materials with Electrical conductivity of 21000000.0 | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip, Wire | |
Electrical resistivity | 3.3e-08 - 5e-08 Ω·m Show Material materials with Electrical resistivity of 3.3e-08 - 5e-08 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chromium | 0.15 - 0.35 % Show Material materials with Chromium of 0.15 - 0.35 % | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip, Wire |
Copper | 0.1 Show Material materials with Copper of 0.1 | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip, Wire |
Iron | 0.4 Show Material materials with Iron of 0.4 | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip, Wire |
Magnesium | 2.2 - 2.8 % Show Material materials with Magnesium of 2.2 - 2.8 % | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip, Wire |
Manganese | 0.1 Show Material materials with Manganese of 0.1 | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip, Wire |
Silicon | 0.25 Show Material materials with Silicon of 0.25 | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip, Wire |
Zinc | 0.1 Show Material materials with Zinc of 0.1 | T6 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | Sheet, Strip, Wire |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |