General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Density | 20.0 °C | 2.71 g/cm³ Show Material materials with Density of 2.71 g/cm³ | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 20.0 °C | 70.0 Show Material materials with Elastic modulus of 70.0 | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip | |
Elongation | 20.0 °C | 6.0 % Show Material materials with Elongation of 6.0 % | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip | A10 |
20.0 °C | 7.0 % Show Material materials with Elongation of 7.0 % | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | A10 | |
20.0 °C | 7.0 % Show Material materials with Elongation of 7.0 % | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip | ||
Hardness, Brinell | 20.0 °C | 80.0 [-] Show Material materials with Hardness, Brinell of 80.0 [-] | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Shear modulus | 20.0 °C | 26.5 Show Material materials with Shear modulus of 26.5 | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip | |
Tensile strength | 20.0 °C | 250.0 - 290.0 MPa Show Material materials with Tensile strength of 250.0 - 290.0 MPa | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | |
20.0 °C | 265.0 - 305.0 MPa Show Material materials with Tensile strength of 265.0 - 305.0 MPa | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Strip |
Thermal
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 2.2e-05 - 2.5e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.2e-05 - 2.5e-05 1/K | Typical for Wrought 5000 Series Aluminium | ||||
Max service temperature | 150.0 °C Show Material materials with Max service temperature of 150.0 °C | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip | Long | |
150.0 °C Show Material materials with Max service temperature of 150.0 °C | Typical for Wrought 5000 Series Aluminium | |||||
Melting point | 560.0 - 655.0 °C Show Material materials with Melting point of 560.0 - 655.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Specific heat capacity | 879.0 - 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 879.0 - 963.0 J/(kg·K) | Typical for Wrought 5000 Series Aluminium | ||||
Thermal conductivity | 20.0 °C | 140.0 - 180.0 W/(m·K) Show Material materials with Thermal conductivity of 140.0 - 180.0 W/(m·K) | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Electrical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Electrical conductivity | 20.0 °C | 20000000.0 - 25000000.0 S/m Show Material materials with Electrical conductivity of 20000000.0 - 25000000.0 S/m | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip | |
Electrical resistivity | 3.3e-08 - 5e-08 Ω·m Show Material materials with Electrical resistivity of 3.3e-08 - 5e-08 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chromium | 0.3 Show Material materials with Chromium of 0.3 | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Copper | 0.1 Show Material materials with Copper of 0.1 | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Iron | 0.5 Show Material materials with Iron of 0.5 | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Magnesium | 1.6 - 2.5 % Show Material materials with Magnesium of 1.6 - 2.5 % | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Manganese | 0.5 - 1.1 % Show Material materials with Manganese of 0.5 - 1.1 % | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Silicon | 0.4 Show Material materials with Silicon of 0.4 | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Titanium | 0.1 Show Material materials with Titanium of 0.1 | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Zinc | 0.2 Show Material materials with Zinc of 0.2 | T6 | DIN 1725-1, EN 573-3, EN 573-4 | Sheet, Flat, Strip |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |