General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Density | 20.0 °C | 2.64 g/cm³ Show Material materials with Density of 2.64 g/cm³ | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 20.0 °C | 72.0 Show Material materials with Elastic modulus of 72.0 | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Shear modulus | 20.0 °C | 27.0 Show Material materials with Shear modulus of 27.0 | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | |
Tensile strength | 20.0 °C | 380.0 - 430.0 MPa Show Material materials with Tensile strength of 380.0 - 430.0 MPa | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Thermal
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 2.2e-05 - 2.5e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.2e-05 - 2.5e-05 1/K | Typical for Wrought 5000 Series Aluminium | ||||
Max service temperature | 150.0 °C Show Material materials with Max service temperature of 150.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Melting point | 560.0 - 655.0 °C Show Material materials with Melting point of 560.0 - 655.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Specific heat capacity | 20.0 °C | 900.0 J/(kg·K) Show Material materials with Specific heat capacity of 900.0 J/(kg·K) | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | |
Thermal conductivity | 20.0 °C | 140.0 Show Material materials with Thermal conductivity of 140.0 | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Electrical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Electrical conductivity | 20.0 °C | 19000000.0 Show Material materials with Electrical conductivity of 19000000.0 | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat | |
Electrical resistivity | 3.3e-08 - 5e-08 Ω·m Show Material materials with Electrical resistivity of 3.3e-08 - 5e-08 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chromium | 0.1 Show Material materials with Chromium of 0.1 | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Copper | 0.15 Show Material materials with Copper of 0.15 | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Iron | 0.35 Show Material materials with Iron of 0.35 | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Magnesium | 4.0 - 5.0 % Show Material materials with Magnesium of 4.0 - 5.0 % | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Manganese | 0.2 - 0.5 % Show Material materials with Manganese of 0.2 - 0.5 % | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Silicon | 0.2 Show Material materials with Silicon of 0.2 | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Titanium | 0.1 Show Material materials with Titanium of 0.1 | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Zinc | 0.25 Show Material materials with Zinc of 0.25 | H18 | DIN 1725-1, EN 573-3, EN 573-4 | Flat |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |