General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Density | 20.0 °C | 2.77 g/cm³ Show Material materials with Density of 2.77 g/cm³ | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 20.0 °C | 68.0 - 70.0 GPa Show Material materials with Elastic modulus of 68.0 - 70.0 GPa | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube | |
Elongation | 20.0 °C | 7.0 % Show Material materials with Elongation of 7.0 % | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Rod | |
20.0 °C | 8.0 % Show Material materials with Elongation of 8.0 % | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Sheet, Strip, Tube, Rod | A10 | |
20.0 °C | 9.0 % Show Material materials with Elongation of 9.0 % | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Sheet | ||
20.0 °C | 10.0 % Show Material materials with Elongation of 10.0 % | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Sheet, Strip, Tube, Rod | ||
Hardness, Brinell | 20.0 °C | 100.0 [-] Show Material materials with Hardness, Brinell of 100.0 [-] | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Rod | |
20.0 °C | 100.0 - 105.0 [-] Show Material materials with Hardness, Brinell of 100.0 - 105.0 [-] | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Rod | ||
20.0 °C | 105.0 [-] Show Material materials with Hardness, Brinell of 105.0 [-] | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Sheet, Strip, Tube, Rod | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium | ||||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | ||||
Shear modulus | 20.0 °C | 25.0 - 27.0 GPa Show Material materials with Shear modulus of 25.0 - 27.0 GPa | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube | |
Tensile strength | 20.0 °C | 340.0 MPa Show Material materials with Tensile strength of 340.0 MPa | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Sheet | |
20.0 °C | 350.0 MPa Show Material materials with Tensile strength of 350.0 MPa | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Sheet, Strip, Tube, Rod |
Thermal
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | -50.0 °C | 2.14e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.14e-05 1/K | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube | |
100.0 °C | 2.31e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.31e-05 1/K | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube | ||
200.0 °C | 2.4e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.4e-05 1/K | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube | ||
300.0 °C | 2.5e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.5e-05 1/K | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube | ||
Melting point | 465.0 - 655.0 °C Show Material materials with Melting point of 465.0 - 655.0 °C | Typical for Wrought 7000 Series Aluminium | ||||
Specific heat capacity | 20.0 °C | 875.0 J/(kg·K) Show Material materials with Specific heat capacity of 875.0 J/(kg·K) | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube | |
Thermal conductivity | 20.0 °C | 130.0 - 160.0 W/(m·K) Show Material materials with Thermal conductivity of 130.0 - 160.0 W/(m·K) | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Electrical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Electrical conductivity | 20.0 °C | 19000000.0 - 23000000.0 S/m Show Material materials with Electrical conductivity of 19000000.0 - 23000000.0 S/m | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube | |
Electrical resistivity | 2.9e-08 - 5.6e-08 Ω·m Show Material materials with Electrical resistivity of 2.9e-08 - 5.6e-08 Ω·m | Typical for Wrought 7000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chromium | 0.1 - 0.35 % Show Material materials with Chromium of 0.1 - 0.35 % | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Copper | 0.2 Show Material materials with Copper of 0.2 | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Iron | 0.4 Show Material materials with Iron of 0.4 | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Magnesium | 1.0 - 1.4 % Show Material materials with Magnesium of 1.0 - 1.4 % | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Manganese | 0.05 - 0.5 % Show Material materials with Manganese of 0.05 - 0.5 % | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Silicon | 0.35 Show Material materials with Silicon of 0.35 | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Zinc | 4.0 - 5.0 % Show Material materials with Zinc of 4.0 - 5.0 % | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Zirconium | 0.08 - 0.2 % Show Material materials with Zirconium of 0.08 - 0.2 % | T8 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.4336-1, WL 3.4336-2 | Profile, Rod, Sheet, Strip, Tube |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |