General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Density | 20.0 °C | 2.78 g/cm³ Show Material materials with Density of 2.78 g/cm³ | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 20.0 °C | 72.0 GPa Show Material materials with Elastic modulus of 72.0 GPa | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Wire | |
Hardness, Brinell | 20.0 °C | 60.0 [-] Show Material materials with Hardness, Brinell of 60.0 [-] | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Wire | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium | ||||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | ||||
Shear modulus | 20.0 °C | 27.5 GPa Show Material materials with Shear modulus of 27.5 GPa | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Wire | |
Tensile strength | 20.0 °C | 200.0 MPa Show Material materials with Tensile strength of 200.0 MPa | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Thermal
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 2.1e-05 - 2.4e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.1e-05 - 2.4e-05 1/K | Typical for Wrought 7000 Series Aluminium | ||||
Melting point | 465.0 - 655.0 °C Show Material materials with Melting point of 465.0 - 655.0 °C | Typical for Wrought 7000 Series Aluminium | ||||
Specific heat capacity | 795.0 - 1050.0 J/(kg·K) Show Material materials with Specific heat capacity of 795.0 - 1050.0 J/(kg·K) | Typical for Wrought 7000 Series Aluminium | ||||
Thermal conductivity | 20.0 °C | 130.0 - 160.0 W/(m·K) Show Material materials with Thermal conductivity of 130.0 - 160.0 W/(m·K) | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Electrical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Electrical conductivity | 20.0 °C | 19000000.0 - 23000000.0 S/m Show Material materials with Electrical conductivity of 19000000.0 - 23000000.0 S/m | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Wire | |
Electrical resistivity | 2.9e-08 - 5.6e-08 Ω·m Show Material materials with Electrical resistivity of 2.9e-08 - 5.6e-08 Ω·m | Typical for Wrought 7000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chromium | 0.1 - 0.3 % Show Material materials with Chromium of 0.1 - 0.3 % | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Copper | 0.5 - 1.0 % Show Material materials with Copper of 0.5 - 1.0 % | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Iron | 0.5 Show Material materials with Iron of 0.5 | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Magnesium | 2.6 - 3.7 % Show Material materials with Magnesium of 2.6 - 3.7 % | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Manganese | 0.1 - 0.4 % Show Material materials with Manganese of 0.1 - 0.4 % | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Silicon | 0.5 Show Material materials with Silicon of 0.5 | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Zinc | 4.3 - 5.2 % Show Material materials with Zinc of 4.3 - 5.2 % | H14 | DIN 1725-1, EN 573-3, EN 573-4 | Wire |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |