General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Density | 20.0 °C | 2.7 g/cm³ Show Material materials with Density of 2.7 g/cm³ | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Wire, Flat |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 68.0 - 70.0 GPa Show Material materials with Elastic modulus of 68.0 - 70.0 GPa | Typical for Wrought 1000 Series Aluminium | ||||
Elongation | 20.0 °C | 2.0 % Show Material materials with Elongation of 2.0 % | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Flat | A10 |
20.0 °C | 3.0 % Show Material materials with Elongation of 3.0 % | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Flat | ||
Hardness, Brinell | 20.0 °C | 40.0 [-] Show Material materials with Hardness, Brinell of 40.0 [-] | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Flat | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | ||||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | ||||
Shear modulus | 20.0 °C | 25.0 - 26.5 GPa Show Material materials with Shear modulus of 25.0 - 26.5 GPa | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Wire, Flat | |
Tensile strength | 20.0 °C | 160.0 MPa Show Material materials with Tensile strength of 160.0 MPa | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Flat, Wire | |
20.0 °C | 170.0 MPa Show Material materials with Tensile strength of 170.0 MPa | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Wire | ||
20.0 °C | 180.0 MPa Show Material materials with Tensile strength of 180.0 MPa | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Wire |
Thermal
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 2.2e-05 - 2.5e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.2e-05 - 2.5e-05 1/K | Typical for Wrought 1000 Series Aluminium | ||||
Melting point | 645.0 - 660.0 °C Show Material materials with Melting point of 645.0 - 660.0 °C | Typical for Wrought 1000 Series Aluminium | ||||
Specific heat capacity | 20.0 °C | 921.0 J/(kg·K) Show Material materials with Specific heat capacity of 921.0 J/(kg·K) | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Wire, Flat | |
Thermal conductivity | 20.0 °C | 230.0 W/(m·K) Show Material materials with Thermal conductivity of 230.0 W/(m·K) | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Wire, Flat |
Electrical
Property | Value | Comment |
---|---|---|
Electrical conductivity | 33000000.0 - 38000000.0 S/m Show Material materials with Electrical conductivity of 33000000.0 - 38000000.0 S/m | Typical for Wrought 1000 Series Aluminium |
Electrical resistivity | 2.7e-08 - 3e-08 Ω·m Show Material materials with Electrical resistivity of 2.7e-08 - 3e-08 Ω·m | Typical for Wrought 1000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Copper | 0.02 Show Material materials with Copper of 0.02 | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Wire, Flat |
Iron | 0.4 Show Material materials with Iron of 0.4 | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Wire, Flat |
Magnesium | 0.05 Show Material materials with Magnesium of 0.05 | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Wire, Flat |
Silicon | 0.25 Show Material materials with Silicon of 0.25 | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Wire, Flat |
Zinc | 0.05 Show Material materials with Zinc of 0.05 | H1x | DIN 1712-3, EN 573-3, EN 573-4 | Wire, Flat |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent | |
Workability | Excellent workability. |