Description

Aluminum EN AW-3003 is a popular alloy that offers customers very good atmospheric corrosion resistance and moderate strength. Aluminum 3003 offers good machinability for aluminum alloys, though it is not heat treatable. Unlike other aluminum alloys, EN AW-3003 is weldable by conventional welding methods. It also takes cold and hot working well and has generally better mechanical properties when compared to 1000 series aluminum alloys.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

2.73 g/cm³

Show Material materials with Density of 2.73 g/cm³

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20.0 °C

2.73 g/cm³

Show Material materials with Density of 2.73 g/cm³

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

69.0 GPa

Show Material materials with Elastic modulus of 69.0 GPa

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

69.5 GPa

Show Material materials with Elastic modulus of 69.5 GPa

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

-270 °C, 20 °C, -270.0 °C, 20.0 °C

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

F

EN 573-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar, Profile, Rod, Flat

300 °C, 300.0 °C

50.0 GPa

Show Material materials with Elastic modulus of 50.0 GPa

F

EN 573-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar, Profile, Rod, Flat

20.0 °C, 50.0 °C

69.0 GPa

Show Material materials with Elastic modulus of 69.0 GPa

F

EN 573-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar, Profile, Rod, Flat

20.0 °C

69.5 GPa

Show Material materials with Elastic modulus of 69.5 GPa

F

EN 573-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar, Profile, Rod, Flat

20.0 °C

60.0 - 70.0 GPa

Show Material materials with Elastic modulus of 60.0 - 70.0 GPa

F

EN 573-3

Profile, Rod, Flat, Tube

20.0 °C

69.5 - 70.0 GPa

Show Material materials with Elastic modulus of 69.5 - 70.0 GPa

F

EN 573-3

Profile, Rod, Flat, Tube

20.0 °C

69.0 - 70.0 GPa

Show Material materials with Elastic modulus of 69.0 - 70.0 GPa

F

EN 573-3

Profile, Rod, Flat, Tube

20.0 °C

65.0 - 70.0 GPa

Show Material materials with Elastic modulus of 65.0 - 70.0 GPa

F

EN 573-3

Profile, Rod, Flat, Tube

20.0 °C

60.0 - 65.0 GPa

Show Material materials with Elastic modulus of 60.0 - 65.0 GPa

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

65.0 - 69.5 GPa

Show Material materials with Elastic modulus of 65.0 - 69.5 GPa

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

65.0 - 69.0 GPa

Show Material materials with Elastic modulus of 65.0 - 69.0 GPa

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

60.0 - 69.5 GPa

Show Material materials with Elastic modulus of 60.0 - 69.5 GPa

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

69.0 - 69.5 GPa

Show Material materials with Elastic modulus of 69.0 - 69.5 GPa

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

60.0 - 69.0 GPa

Show Material materials with Elastic modulus of 60.0 - 69.0 GPa

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

100.0 °C

68.0 GPa

Show Material materials with Elastic modulus of 68.0 GPa

F

EN 573-3

Profile, Rod, Flat, Tube

150.0 °C

66.0 GPa

Show Material materials with Elastic modulus of 66.0 GPa

F

EN 573-3

Profile, Rod, Flat, Tube

200.0 °C

63.0 GPa

Show Material materials with Elastic modulus of 63.0 GPa

F

EN 573-3

Profile, Rod, Flat, Tube

250.0 °C

57.0 GPa

Show Material materials with Elastic modulus of 57.0 GPa

F

EN 573-3

Profile, Rod, Flat, Tube

Elongation

20.0 °C

20.0 %

Show Material materials with Elongation of 20.0 %

F

EN 573-3

Profile, Rod, Tube

A50

20.0 %

Show Material materials with Elongation of 20.0 %

F

EN 573-3, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

A50

20.0 °C

25.0 %

Show Material materials with Elongation of 25.0 %

F

EN 573-3

Rod, Tube, Profile

20.0 °C

12.0 %

Show Material materials with Elongation of 12.0 %

F

EN 573-3

Rod, Profile

12.0 %

Show Material materials with Elongation of 12.0 %

F

EN 573-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

25.0 %

Show Material materials with Elongation of 25.0 %

F

EN 573-3, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

A100

Unlock all property charts

Hardness, Brinell

20.0 °C

30.0 [-]

Show Material materials with Hardness, Brinell of 30.0 [-]

F

EN 573-3

Profile, Rod, Tube

33.0 [-]

Show Material materials with Hardness, Brinell of 33.0 [-]

F

EN 573-3, EN 570

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 3000 Series Aluminium

Poisson's ratio

20.0 °C

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

Shear modulus

26.1 GPa

Show Material materials with Shear modulus of 26.1 GPa

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20.0 °C

24.0 - 26.5 GPa

Show Material materials with Shear modulus of 24.0 - 26.5 GPa

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

26.1 - 26.5 GPa

Show Material materials with Shear modulus of 26.1 - 26.5 GPa

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

24.0 - 26.1 GPa

Show Material materials with Shear modulus of 24.0 - 26.1 GPa

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

26.1 GPa

Show Material materials with Shear modulus of 26.1 GPa

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

Unlock all property charts

Tensile strength

20.0 °C

95.0 MPa

Show Material materials with Tensile strength of 95.0 MPa

F

EN 573-3

Rod, Tube, Profile, Flat

20.0 °C

160.0 MPa

Show Material materials with Tensile strength of 160.0 MPa

F

EN 573-3

Rod, Profile

160.0 MPa

Show Material materials with Tensile strength of 160.0 MPa

F

EN 573-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

120.0 - 220.0 MPa

Show Material materials with Tensile strength of 120.0 - 220.0 MPa

F

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

95.0 MPa

Show Material materials with Tensile strength of 95.0 MPa

F

EN 573-3, EN 485, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20.0 °C

95.0 MPa

Show Material materials with Tensile strength of 95.0 MPa

F

EN 573-3

Flat

Transverse

Unlock all property charts

Thermal

PropertyTemperatureValueConditionRelated StandardsShape

Coefficient of thermal expansion

100 °C, 20 °C

2.3199999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3199999999999998e-05 1/K

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

300 °C, 20 °C, 300.0 °C

2.52e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.52e-05 1/K

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar, Profile, Rod, Flat

200 °C, 20 °C, 200.0 °C

2.41e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.41e-05 1/K

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar, Profile, Rod, Flat

20 °C, -50 °C

2.1499999999999997e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.1499999999999997e-05 1/K

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

-50.0 °C

2.15e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.15e-05 1/K

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

100.0 °C

2.32e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.32e-05 1/K

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

Unlock all property charts

Melting point

640.0 - 655.0 °C

Show Material materials with Melting point of 640.0 - 655.0 °C

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

643.0 - 654.0 °C

Show Material materials with Melting point of 643.0 - 654.0 °C

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Specific heat capacity

893.0 J/(kg·K)

Show Material materials with Specific heat capacity of 893.0 J/(kg·K)

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20.0 °C

893.0 J/(kg·K)

Show Material materials with Specific heat capacity of 893.0 J/(kg·K)

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

892.0 - 893.0 J/(kg·K)

Show Material materials with Specific heat capacity of 892.0 - 893.0 J/(kg·K)

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

892.0 J/(kg·K)

Show Material materials with Specific heat capacity of 892.0 J/(kg·K)

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

Unlock all property charts

Thermal conductivity

159.0 - 193.0 W/(m·K)

Show Material materials with Thermal conductivity of 159.0 - 193.0 W/(m·K)

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20.0 °C

160.0 - 200.0 W/(m·K)

Show Material materials with Thermal conductivity of 160.0 - 200.0 W/(m·K)

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar, Profile, Rod, Flat

20.0 °C

160.0 W/(m·K)

Show Material materials with Thermal conductivity of 160.0 W/(m·K)

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

Unlock all property charts

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical conductivity

24000000.0 - 29000000.0 S/m

Show Material materials with Electrical conductivity of 24000000.0 - 29000000.0 S/m

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20.0 °C

23000000.0 - 29000000.0 S/m

Show Material materials with Electrical conductivity of 23000000.0 - 29000000.0 S/m

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar, Profile, Rod, Flat

20.0 °C

22000000.0 - 29000000.0 S/m

Show Material materials with Electrical conductivity of 22000000.0 - 29000000.0 S/m

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

Unlock all property charts

Electrical resistivity

3.45e-08 - 4.17e-08 Ω·m

Show Material materials with Electrical resistivity of 3.45e-08 - 4.17e-08 Ω·m

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

3.45e-08 - 4.35e-08 Ω·m

Show Material materials with Electrical resistivity of 3.45e-08 - 4.35e-08 Ω·m

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20.0 °C

4.1e-08 Ω·m

Show Material materials with Electrical resistivity of 4.1e-08 Ω·m

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

3.4e-08 - 4.1e-08 Ω·m

Show Material materials with Electrical resistivity of 3.4e-08 - 4.1e-08 Ω·m

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

4.1e-08 - 4.5e-08 Ω·m

Show Material materials with Electrical resistivity of 4.1e-08 - 4.5e-08 Ω·m

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

20.0 °C

3.4e-08 - 4.5e-08 Ω·m

Show Material materials with Electrical resistivity of 3.4e-08 - 4.5e-08 Ω·m

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

Unlock all property charts

Chemical properties

PropertyValueConditionRelated StandardsShape

Copper

0.05 - 0.2 %

Show Material materials with Copper of 0.05 - 0.2 %

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Foil, Wire, Bar

Iron

0.7 %

Show Material materials with Iron of 0.7 %

F

EN 573-3

Profile, Rod, Flat, Tube, Plate

0.70 %

Show Material materials with Iron of 0.70 %

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Manganese

1.0 - 1.5 %

Show Material materials with Manganese of 1.0 - 1.5 %

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Foil, Wire, Bar

Silicon

0.6 %

Show Material materials with Silicon of 0.6 %

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Foil, Wire, Bar

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

F

EN 573-3, EN 1386, EN 1715-3, EN 485, EN 570, EN 755

Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Foil, Wire, Bar

Technological properties

Property
Anodizing

decorative: sufficient, Protective: very good

Brazing

hard brazing (with flux/ without flux): very good / very good, friction soldering: very good, soft brazing with flux: very good

Corrosion properties

Seawater: good, weathering: very good

Workability