Aluminum EN AW-3003 is a popular alloy that offers customers very good atmospheric corrosion resistance and moderate strength. Aluminum 3003 offers good machinability for aluminum alloys, though it is not heat treatable. Unlike other aluminum alloys, EN AW-3003 is weldable by conventional welding methods. It also takes cold and hot working well and has generally better mechanical properties when compared to 1000 series aluminum alloys.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

20.0 °C

2.73 g/cm³

Show Material materials with Density of 2.73 g/cm³

H15

EN 573-3

Tube

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

-270.0 °C

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

H15

EN 573-3

Tube

20.0 °C

60.0 - 70.0 GPa

Show Material materials with Elastic modulus of 60.0 - 70.0 GPa

H15

EN 573-3

Tube

20.0 °C

60.0 - 65.0 GPa

Show Material materials with Elastic modulus of 60.0 - 65.0 GPa

H15

EN 573-3

Tube

20.0 °C

60.0 - 69.5 GPa

Show Material materials with Elastic modulus of 60.0 - 69.5 GPa

H15

EN 573-3

Tube

20.0 °C

60.0 - 69.0 GPa

Show Material materials with Elastic modulus of 60.0 - 69.0 GPa

H15

EN 573-3

Tube

20.0 °C

65.0 - 70.0 GPa

Show Material materials with Elastic modulus of 65.0 - 70.0 GPa

H15

EN 573-3

Tube

20.0 °C

65.0 - 69.5 GPa

Show Material materials with Elastic modulus of 65.0 - 69.5 GPa

H15

EN 573-3

Tube

20.0 °C

65.0 - 69.0 GPa

Show Material materials with Elastic modulus of 65.0 - 69.0 GPa

H15

EN 573-3

Tube

20.0 °C

69.0 - 70.0 GPa

Show Material materials with Elastic modulus of 69.0 - 70.0 GPa

H15

EN 573-3

Tube

20.0 °C

69.0 - 69.5 GPa

Show Material materials with Elastic modulus of 69.0 - 69.5 GPa

H15

EN 573-3

Tube

20.0 °C

69.0 GPa

Show Material materials with Elastic modulus of 69.0 GPa

H15

EN 573-3

Tube

20.0 °C

69.5 - 70.0 GPa

Show Material materials with Elastic modulus of 69.5 - 70.0 GPa

H15

EN 573-3

Tube

20.0 °C

69.5 GPa

Show Material materials with Elastic modulus of 69.5 GPa

H15

EN 573-3

Tube

20.0 °C

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

H15

EN 573-3

Tube

50.0 °C

69.0 GPa

Show Material materials with Elastic modulus of 69.0 GPa

H15

EN 573-3

Tube

100.0 °C

68.0 GPa

Show Material materials with Elastic modulus of 68.0 GPa

H15

EN 573-3

Tube

150.0 °C

66.0 GPa

Show Material materials with Elastic modulus of 66.0 GPa

H15

EN 573-3

Tube

200.0 °C

63.0 GPa

Show Material materials with Elastic modulus of 63.0 GPa

H15

EN 573-3

Tube

250.0 °C

57.0 GPa

Show Material materials with Elastic modulus of 57.0 GPa

H15

EN 573-3

Tube

300.0 °C

50.0 GPa

Show Material materials with Elastic modulus of 50.0 GPa

H15

EN 573-3

Tube

Elongation

20.0 °C

4.0 %

Show Material materials with Elongation of 4.0 %

H15

EN 573-3

Tube

A50

20.0 °C

5.0 %

Show Material materials with Elongation of 5.0 %

H15

EN 573-3

Tube

Hardness, Brinell

20.0 °C

44.0 [-]

Show Material materials with Hardness, Brinell of 44.0 [-]

H15

EN 573-3

Tube

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 3000 Series Aluminium

Poisson's ratio

20.0 °C

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

H15

EN 573-3

Tube

Shear modulus

20.0 °C

24.0 - 26.5 GPa

Show Material materials with Shear modulus of 24.0 - 26.5 GPa

H15

EN 573-3

Tube

20.0 °C

24.0 - 26.1 GPa

Show Material materials with Shear modulus of 24.0 - 26.1 GPa

H15

EN 573-3

Tube

20.0 °C

26.1 - 26.5 GPa

Show Material materials with Shear modulus of 26.1 - 26.5 GPa

H15

EN 573-3

Tube

20.0 °C

26.1 GPa

Show Material materials with Shear modulus of 26.1 GPa

H15

EN 573-3

Tube

Tensile strength

20.0 °C

145.0 - 180.0 MPa

Show Material materials with Tensile strength of 145.0 - 180.0 MPa

H15

EN 573-3

Tube

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

-50.0 °C

2.15e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.15e-05 1/K

H15

EN 573-3

Tube

100.0 °C

2.32e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.32e-05 1/K

H15

EN 573-3

Tube

200.0 °C

2.41e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.41e-05 1/K

H15

EN 573-3

Tube

300.0 °C

2.52e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.52e-05 1/K

H15

EN 573-3

Tube

Melting point

629.0 - 654.0 °C

Show Material materials with Melting point of 629.0 - 654.0 °C

Typical for Wrought 3000 Series Aluminium

Specific heat capacity

20.0 °C

892.0 - 893.0 J/(kg·K)

Show Material materials with Specific heat capacity of 892.0 - 893.0 J/(kg·K)

H15

EN 573-3

Tube

20.0 °C

892.0 J/(kg·K)

Show Material materials with Specific heat capacity of 892.0 J/(kg·K)

H15

EN 573-3

Tube

20.0 °C

893.0 J/(kg·K)

Show Material materials with Specific heat capacity of 893.0 J/(kg·K)

H15

EN 573-3

Tube

Thermal conductivity

20.0 °C

160.0 - 200.0 W/(m·K)

Show Material materials with Thermal conductivity of 160.0 - 200.0 W/(m·K)

H15

EN 573-3

Tube

20.0 °C

160.0 W/(m·K)

Show Material materials with Thermal conductivity of 160.0 W/(m·K)

H15

EN 573-3

Tube

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical conductivity

20.0 °C

22000000.0 - 29000000.0 S/m

Show Material materials with Electrical conductivity of 22000000.0 - 29000000.0 S/m

H15

EN 573-3

Tube

20.0 °C

23000000.0 - 29000000.0 S/m

Show Material materials with Electrical conductivity of 23000000.0 - 29000000.0 S/m

H15

EN 573-3

Tube

Electrical resistivity

20.0 °C

3.4e-08 - 4.1e-08 Ω·m

Show Material materials with Electrical resistivity of 3.4e-08 - 4.1e-08 Ω·m

H15

EN 573-3

Tube

20.0 °C

3.4e-08 - 4.5e-08 Ω·m

Show Material materials with Electrical resistivity of 3.4e-08 - 4.5e-08 Ω·m

H15

EN 573-3

Tube

20.0 °C

4.1e-08 Ω·m

Show Material materials with Electrical resistivity of 4.1e-08 Ω·m

H15

EN 573-3

Tube

20.0 °C

4.1e-08 - 4.5e-08 Ω·m

Show Material materials with Electrical resistivity of 4.1e-08 - 4.5e-08 Ω·m

H15

EN 573-3

Tube

Chemical properties

PropertyValueConditionRelated StandardsShape

Copper

0.05 - 0.2 %

Show Material materials with Copper of 0.05 - 0.2 %

H15

EN 573-3

Tube

Iron

0.7

Show Material materials with Iron of 0.7

H15

EN 573-3

Tube

Manganese

1.0 - 1.5 %

Show Material materials with Manganese of 1.0 - 1.5 %

H15

EN 573-3

Tube

Silicon

0.6

Show Material materials with Silicon of 0.6

H15

EN 573-3

Tube

Zinc

0.1

Show Material materials with Zinc of 0.1

H15

EN 573-3

Tube

Technological properties

Property
Workability

Good workability.