Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

2.00E+7 - 2.40E+7 S/m

Show Material materials with Electrical conductivity of 2.00E+7 - 2.40E+7 S/m

General

PropertyTemperatureValue

Density

20.0 °C

2.72 g/cm³

Show Material materials with Density of 2.72 g/cm³

Mechanical

PropertyTemperatureValue

Elongation

20.0 °C

25 - 90 %

Show Material materials with Elongation of 25 - 90 %

Tensile strength

20.0 °C

35 - 290 MPa

Show Material materials with Tensile strength of 35 - 290 MPa

Yield strength Rp0.2

20.0 °C

20 - 90 MPa

Show Material materials with Yield strength Rp0.2 of 20 - 90 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

-50.0 °C

2.15E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.15E-5 1/K

100.0 °C

2.32E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.32E-5 1/K

200.0 °C

2.41E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.41E-5 1/K

300.0 °C

2.51E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.51E-5 1/K

Melting point

650 °C

Show Material materials with Melting point of 650 °C

Specific heat capacity

20.0 °C

893 J/(kg·K)

Show Material materials with Specific heat capacity of 893 J/(kg·K)

Thermal conductivity

20.0 °C

160 - 190 W/(m·K)

Show Material materials with Thermal conductivity of 160 - 190 W/(m·K)

Chemical properties

PropertyValue

Copper

0.25 %

Show Material materials with Copper of 0.25 %

Iron

0.7 %

Show Material materials with Iron of 0.7 %

Magnesium

0.8 - 1.3 %

Show Material materials with Magnesium of 0.8 - 1.3 %

Manganese

1 - 1.5 %

Show Material materials with Manganese of 1 - 1.5 %

Silicon

0.3 %

Show Material materials with Silicon of 0.3 %

Zinc

0.25 %

Show Material materials with Zinc of 0.25 %