General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Density | 2.71 g/cm³ Show Material materials with Density of 2.71 g/cm³ | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet |
2.71 g/cm³ Show Material materials with Density of 2.71 g/cm³ | H24 | EN 573-3, EN 541 | Strip, Sheet, Plate |
Dimension
Property | Value | Condition | Related Standards | Thickness | Shape |
---|---|---|---|---|---|
Thickness | 0.18 mm Show Material materials with Thickness of 0.18 mm | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | 0.18 mm | Coil, Sheet |
1.0 mm Show Material materials with Thickness of 1.0 mm | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | 1.0 mm | Coil, Sheet |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Bending angle 180° | 2.5 °/t Show Material materials with Bending angle 180° of 2.5 °/t | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | ||
Elastic modulus | 69.0 GPa Show Material materials with Elastic modulus of 69.0 GPa | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | ||
Hardness, HBW | 48 [-] Show Material materials with Hardness, HBW of 48 [-] | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium | ||||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 3000 Series Aluminium | ||||
Shear modulus | 26.0 GPa Show Material materials with Shear modulus of 26.0 GPa | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | ||
Tensile strength | 150.0 - 240.0 MPa Show Material materials with Tensile strength of 150.0 - 240.0 MPa | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | ||
20.0 °C | 150.0 - 190.0 MPa Show Material materials with Tensile strength of 150.0 - 190.0 MPa | H24 | EN 573-3, EN 541 | Sheet, Strip, Plate | ||
Yield strength | 120.0 - 220.0 MPa Show Material materials with Yield strength of 120.0 - 220.0 MPa | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | ||
20.0 °C | 120.0 - 160.0 MPa Show Material materials with Yield strength of 120.0 - 160.0 MPa | H24 | EN 573-3, EN 541 | Sheet, Strip, Plate | RP02 |
Thermal
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 100 °C | 0.000024 1/K Show Material materials with Coefficient of thermal expansion of 0.000024 1/K | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | 20-100°C |
Melting point | 629.0 - 654.0 °C Show Material materials with Melting point of 629.0 - 654.0 °C | Typical for Wrought 3000 Series Aluminium | ||||
Specific heat capacity | 893.0 - 920.0 J/(kg·K) Show Material materials with Specific heat capacity of 893.0 - 920.0 J/(kg·K) | Typical for Wrought 3000 Series Aluminium | ||||
Thermal conductivity | 172 W/(m·K) Show Material materials with Thermal conductivity of 172 W/(m·K) | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet |
Electrical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Electrical conductivity | 23000000.0 - 29000000.0 S/m Show Material materials with Electrical conductivity of 23000000.0 - 29000000.0 S/m | Typical for Wrought 3000 Series Aluminium | |||
Electrical resistivity | 3.7999999999999996e-08 Ω·m Show Material materials with Electrical resistivity of 3.7999999999999996e-08 Ω·m | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chromium | 0.2 % Show Material materials with Chromium of 0.2 % | H24 | EN 573-3, EN 541 | Sheet, Strip, Plate |
0.2 % Show Material materials with Chromium of 0.2 % | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |
Copper | 0.3 % Show Material materials with Copper of 0.3 % | H24 | EN 573-3, EN 541 | Sheet, Strip, Plate |
0.3 % Show Material materials with Copper of 0.3 % | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |
Iron | 0.7 % Show Material materials with Iron of 0.7 % | H24 | EN 573-3 | Sheet |
0.7 % Show Material materials with Iron of 0.7 % | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |
0.70 % Show Material materials with Iron of 0.70 % | H24 | EN 573-3, EN 541 | Strip, Sheet, Plate | |
Magnesium | 0.2 - 0.8 % Show Material materials with Magnesium of 0.2 - 0.8 % | H24 | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541, EN 541 | Sheet, Coil, Sheet, Strip, Plate |
Manganese | 0.3 - 0.8 % Show Material materials with Manganese of 0.3 - 0.8 % | H24 | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541, EN 541 | Sheet, Coil, Sheet, Strip, Plate |
Silicon | 0.6 % Show Material materials with Silicon of 0.6 % | H24 | EN 573-3, EN 541 | Sheet, Strip, Plate |
0.6 % Show Material materials with Silicon of 0.6 % | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |
Titanium | 0.1 % Show Material materials with Titanium of 0.1 % | H24 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | H24 | EN 573-3, EN 541 | Sheet, Strip, Plate |
0.25 % Show Material materials with Zinc of 0.25 % | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet |
Technological properties
Property | ||
---|---|---|
Anodizing | Good | |
Application areas | Closures: Short cups; Food can: Body, Lids; Semi-rigid and corrugated: Pet food | |
Brazing | Good | |
Corrosion properties | Very Good | |
Welding | Very Good | |
Workability | Very Good |