EN 573-3 Grade AW-5019 H34

Want to keep this datasheet? Save it now in your required format

Description

Naturally hard AlMg alloy. The alloy is food safe.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

2.64 g/cm³

Show Material materials with Density of 2.64 g/cm³

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

20.0 °C

2.64 g/cm³

Show Material materials with Density of 2.64 g/cm³

H34

EN 573-3

Rod, Tube, Wire

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

Elongation

3.0 %

Show Material materials with Elongation of 3.0 %

H34

EN 573-3, EN 754

Rod, Tube, Wire

A50

4.0 %

Show Material materials with Elongation of 4.0 %

H34

EN 573-3, EN 754

Rod, Tube, Wire

A100

8.0 %

Show Material materials with Elongation of 8.0 %

H34

EN 573-3, EN 1301

Rod, Tube, Wire

20.0 °C

3.0 %

Show Material materials with Elongation of 3.0 %

H34

EN 573-3

Rod, Tube

A50

20.0 °C

4.0 %

Show Material materials with Elongation of 4.0 %

H34

EN 573-3

Rod, Tube

20.0 °C

8.0 %

Show Material materials with Elongation of 8.0 %

H34

EN 573-3

Wire

A100

Hardness, Brinell

20.0 °C

95.0 [-]

Show Material materials with Hardness, Brinell of 95.0 [-]

H34

EN 573-3

Rod, Tube

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 5000 Series Aluminium

Shear modulus

20.0 °C

27.0 GPa

Show Material materials with Shear modulus of 27.0 GPa

H34

EN 573-3

Rod, Tube, Wire

Tensile strength

300.0 MPa

Show Material materials with Tensile strength of 300.0 MPa

H34

EN 573-3, EN 754

Rod, Tube, Wire

20.0 °C

300.0 MPa

Show Material materials with Tensile strength of 300.0 MPa

H34

EN 573-3

Rod

20.0 °C

300.0 - 380.0 MPa

Show Material materials with Tensile strength of 300.0 - 380.0 MPa

H34

EN 573-3, EN 754

Tube, Rod, Wire

20.0 °C

310.0 - 370.0 MPa

Show Material materials with Tensile strength of 310.0 - 370.0 MPa

H34

EN 573-3, EN 1301

Wire, Rod, Tube

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

-50 °C

2.2499999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.2499999999999998e-05 1/K

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

-50.0 °C

2.25e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.25e-05 1/K

H34

EN 573-3

Rod, Tube, Wire

20 °C

2.2499999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.2499999999999998e-05 1/K

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

20 °C

2.41e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.41e-05 1/K

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

20 °C

2.51e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.51e-05 1/K

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

20 °C

2.61e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.61e-05 1/K

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

100 °C

2.41e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.41e-05 1/K

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

100.0 °C

2.41e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.41e-05 1/K

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

200 °C

2.51e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.51e-05 1/K

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

200.0 °C

2.51e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.51e-05 1/K

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

300 °C

2.61e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.61e-05 1/K

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

300.0 °C

2.61e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.61e-05 1/K

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

Max service temperature

150.0 °C

Show Material materials with Max service temperature of 150.0 °C

Typical for Wrought 5000 Series Aluminium

Melting point

575.0 - 630.0 °C

Show Material materials with Melting point of 575.0 - 630.0 °C

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

Specific heat capacity

904.0 J/(kg·K)

Show Material materials with Specific heat capacity of 904.0 J/(kg·K)

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

20.0 °C

904.0 J/(kg·K)

Show Material materials with Specific heat capacity of 904.0 J/(kg·K)

H34

EN 573-3

Rod, Tube, Wire

Thermal conductivity

20.0 °C

110.0 - 140.0 W/(m·K)

Show Material materials with Thermal conductivity of 110.0 - 140.0 W/(m·K)

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical conductivity

20.0 °C

15000000.0 - 19000000.0 S/m

Show Material materials with Electrical conductivity of 15000000.0 - 19000000.0 S/m

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

Electrical resistivity

5.26e-08 - 6.67e-08 Ω·m

Show Material materials with Electrical resistivity of 5.26e-08 - 6.67e-08 Ω·m

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

Chemical properties

PropertyValueConditionRelated StandardsShape

Chromium

0.2 %

Show Material materials with Chromium of 0.2 %

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

Copper

0.1 %

Show Material materials with Copper of 0.1 %

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

Iron

0.5 %

Show Material materials with Iron of 0.5 %

H34

EN 573-3

Rod, Tube, Wire

0.50 %

Show Material materials with Iron of 0.50 %

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

Magnesium

4.5 - 5.6 %

Show Material materials with Magnesium of 4.5 - 5.6 %

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

Manganese

0.1 - 0.6 %

Show Material materials with Manganese of 0.1 - 0.6 %

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

Titanium

0.2 %

Show Material materials with Titanium of 0.2 %

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

Zinc

0.2 %

Show Material materials with Zinc of 0.2 %

H34

EN 573-3, EN 1301, EN 754

Rod, Tube, Wire

Technological properties

Property
Anodizing

decorative: sufficient, Protective: very good

Brazing

hard brazing (with flux/ without flux): poor / poor, friction soldering: acceptable, soft brazing with flux: poor

Corrosion properties

Seawater: very good, weathering: very good

Workability

Bending / Spinning (cold): good / sufficient, Impact extrusion (cold): poor, Deep drawing / upsetting (Condition) good (O) / good (O)