General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Density | 2.72 g/cm³ Show Material materials with Density of 2.72 g/cm³ | H36 | EN 573-3, EN 1592, EN 485 | Strip, Sheet, Plate, Welded Tube |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 69.0 - 70.0 GPa Show Material materials with Elastic modulus of 69.0 - 70.0 GPa | Typical for Wrought 5000 Series Aluminium | ||||
Hardness, Brinell | 74.0 [-] Show Material materials with Hardness, Brinell of 74.0 [-] | H36 | EN 573-3, EN 485 | Strip, Sheet, Plate, Welded Tube | ||
20.0 °C | 74.0 [-] Show Material materials with Hardness, Brinell of 74.0 [-] | H36 | EN 573-3 | Flat | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Shear modulus | 26.0 - 26.5 GPa Show Material materials with Shear modulus of 26.0 - 26.5 GPa | Typical for Wrought 5000 Series Aluminium | ||||
Tensile strength | 230.0 MPa Show Material materials with Tensile strength of 230.0 MPa | H36 | EN 573-3, EN 1592 | Strip, Sheet, Plate, Welded Tube | ||
20.0 °C | 240.0 - 280.0 MPa Show Material materials with Tensile strength of 240.0 - 280.0 MPa | H36 | EN 573-3 | Flat | Transverse | |
20.0 °C | 240.0 - 280.0 MPa Show Material materials with Tensile strength of 240.0 - 280.0 MPa | H36 | EN 573-3, EN 485 | Strip, Sheet, Plate, Welded Tube, Flat |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 2.2e-05 - 2.5e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.2e-05 - 2.5e-05 1/K | Typical for Wrought 5000 Series Aluminium |
Max service temperature | 150.0 °C Show Material materials with Max service temperature of 150.0 °C | Typical for Wrought 5000 Series Aluminium |
Melting point | 560.0 - 655.0 °C Show Material materials with Melting point of 560.0 - 655.0 °C | Typical for Wrought 5000 Series Aluminium |
Specific heat capacity | 879.0 - 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 879.0 - 963.0 J/(kg·K) | Typical for Wrought 5000 Series Aluminium |
Thermal conductivity | 112.0 - 205.0 W/(m·K) Show Material materials with Thermal conductivity of 112.0 - 205.0 W/(m·K) | Typical for Wrought 5000 Series Aluminium |
Electrical
Property | Value | Comment |
---|---|---|
Electrical conductivity | 18000000.0 - 31000000.0 S/m Show Material materials with Electrical conductivity of 18000000.0 - 31000000.0 S/m | Typical for Wrought 5000 Series Aluminium |
Electrical resistivity | 3.3e-08 - 5e-08 Ω·m Show Material materials with Electrical resistivity of 3.3e-08 - 5e-08 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chromium | 0.1 - 0.3 % Show Material materials with Chromium of 0.1 - 0.3 % | H36 | EN 573-3, EN 1592, EN 485 | Flat, Strip, Sheet, Plate, Welded Tube |
Copper | 0.25 % Show Material materials with Copper of 0.25 % | H36 | EN 573-3, EN 1592, EN 485 | Flat, Strip, Sheet, Plate, Welded Tube |
Iron | 0.7 % Show Material materials with Iron of 0.7 % | H36 | EN 573-3 | Flat |
0.70 % Show Material materials with Iron of 0.70 % | H36 | EN 573-3, EN 1592, EN 485 | Strip, Sheet, Plate, Welded Tube | |
Magnesium | 1.0 - 1.5 % Show Material materials with Magnesium of 1.0 - 1.5 % | H36 | EN 573-3, EN 1592, EN 485 | Flat, Strip, Sheet, Plate, Welded Tube |
Manganese | 0.9 - 1.4 % Show Material materials with Manganese of 0.9 - 1.4 % | H36 | EN 573-3, EN 1592, EN 485 | Flat, Strip, Sheet, Plate, Welded Tube |
Silicon | 0.3 % Show Material materials with Silicon of 0.3 % | H36 | EN 573-3, EN 1592, EN 485 | Flat, Strip, Sheet, Plate, Welded Tube |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | H36 | EN 573-3, EN 1592, EN 485 | Flat, Strip, Sheet, Plate, Welded Tube |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |