EN 573-3 Grade AW-2014A T4511

Want to keep this datasheet? Save it now in your required format

Description

The material EN AW-AlCu4SiMg(A) is produced for extruded and drawn components, wire and prewire for mechanical applications. The alloy is used for sheet, strip, forged parts and prematerial. It is not food-safe.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated StandardsShape

Density

2.8 g/cm³

Show Material materials with Density of 2.8 g/cm³

T4511

EN 573-3, EN 754, EN 755

Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

73.0 GPa

Show Material materials with Elastic modulus of 73.0 GPa

T4511

EN 573-3, EN 754, EN 755

Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire

Elongation

8.0 %

Show Material materials with Elongation of 8.0 %

T4511

EN 573-3, EN 754

Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire

A50

8.0 %

Show Material materials with Elongation of 8.0 %

T4511

EN 573-3, EN 755

Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire

A100

10.0 %

Show Material materials with Elongation of 10.0 %

T4511

EN 573-3, EN 755

Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire

A50

10.0 %

Show Material materials with Elongation of 10.0 %

T4511

EN 573-3, EN 754, EN 755

Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire

A100

11.0 %

Show Material materials with Elongation of 11.0 %

T4511

EN 573-3, EN 755

Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire

A50

11.0 %

Show Material materials with Elongation of 11.0 %

T4511

EN 573-3, EN 755

Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire

A100

12.0 %

Show Material materials with Elongation of 12.0 %

T4511

EN 573-3, EN 755

Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire

A100

13.0 %

Show Material materials with Elongation of 13.0 %

T4511

EN 573-3, EN 755

Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire

A100

20.0 °C

8.0 %

Show Material materials with Elongation of 8.0 %

T4511

EN 573-3

Tube

A50

20.0 °C

8.0 %

Show Material materials with Elongation of 8.0 %

T4511

EN 573-3

Rod

20.0 °C

10.0 %

Show Material materials with Elongation of 10.0 %

T4511

EN 573-3

Tube, Profile

A50

20.0 °C

10.0 %

Show Material materials with Elongation of 10.0 %

T4511

EN 573-3

Tube, Profile, Rod

20.0 °C

11.0 %

Show Material materials with Elongation of 11.0 %

T4511

EN 573-3

Rod

A50

20.0 °C

11.0 %

Show Material materials with Elongation of 11.0 %

T4511

EN 573-3

Tube, Profile

20.0 °C

12.0 %

Show Material materials with Elongation of 12.0 %

T4511

EN 573-3

Rod

20.0 °C

13.0 %

Show Material materials with Elongation of 13.0 %

T4511

EN 573-3

Rod

Hardness, Brinell

20.0 °C

110.0 [-]

Show Material materials with Hardness, Brinell of 110.0 [-]

T4511

EN 573-3

Profile, Rod, Tube

20.0 °C

110.0 - 140.0 [-]

Show Material materials with Hardness, Brinell of 110.0 - 140.0 [-]

T4511

EN 573-3

Rod

20.0 °C

140.0 [-]

Show Material materials with Hardness, Brinell of 140.0 [-]

T4511

EN 573-3

Rod

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 2000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 2000 Series Aluminium

Shear modulus

27.4 GPa

Show Material materials with Shear modulus of 27.4 GPa

T4511

EN 573-3, EN 754, EN 755

Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire

Tensile strength

350.0 MPa

Show Material materials with Tensile strength of 350.0 MPa

T4511

EN 573-3, EN 755

Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire

370.0 MPa

Show Material materials with Tensile strength of 370.0 MPa

T4511

EN 573-3, EN 755

Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire

380.0 MPa

Show Material materials with Tensile strength of 380.0 MPa

T4511

EN 573-3, EN 754

Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire

390.0 MPa

Show Material materials with Tensile strength of 390.0 MPa

T4511

EN 573-3, EN 755

Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire

410.0 MPa

Show Material materials with Tensile strength of 410.0 MPa

T4511

EN 573-3, EN 755

Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire

20.0 °C

350.0 MPa

Show Material materials with Tensile strength of 350.0 MPa

T4511

EN 573-3

Rod

20.0 °C

370.0 MPa

Show Material materials with Tensile strength of 370.0 MPa

T4511

EN 573-3

Tube, Profile, Rod

20.0 °C

380.0 MPa

Show Material materials with Tensile strength of 380.0 MPa

T4511

EN 573-3

Tube

20.0 °C

390.0 MPa

Show Material materials with Tensile strength of 390.0 MPa

T4511

EN 573-3

Rod

20.0 °C

410.0 MPa

Show Material materials with Tensile strength of 410.0 MPa

T4511

EN 573-3

Profile, Rod

Thermal

PropertyValueComment

Coefficient of thermal expansion

1.6e-05 - 2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.6e-05 - 2.4e-05 1/K

Typical for Wrought 2000 Series Aluminium

Melting point

500.0 - 650.0 °C

Show Material materials with Melting point of 500.0 - 650.0 °C

Typical for Wrought 2000 Series Aluminium

Specific heat capacity

816.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 816.0 - 963.0 J/(kg·K)

Typical for Wrought 2000 Series Aluminium

Thermal conductivity

112.0 - 251.0 W/(m·K)

Show Material materials with Thermal conductivity of 112.0 - 251.0 W/(m·K)

Typical for Wrought 2000 Series Aluminium

Electrical

PropertyValueComment

Electrical conductivity

18000000.0 - 30000000.0 S/m

Show Material materials with Electrical conductivity of 18000000.0 - 30000000.0 S/m

Typical for Wrought 2000 Series Aluminium

Electrical resistivity

3.4e-08 - 6e-08 Ω·m

Show Material materials with Electrical resistivity of 3.4e-08 - 6e-08 Ω·m

Typical for Wrought 2000 Series Aluminium

Chemical properties

PropertyValueConditionRelated StandardsShape

Beryllium

0.0001 - 0.005 %

Show Material materials with Beryllium of 0.0001 - 0.005 %

T4511

EN 573-3, EN 754, EN 755

Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire

Chromium

0.1 %

Show Material materials with Chromium of 0.1 %

T4511

EN 573-3, EN 754, EN 755

Tube, Profile, Rod, Strip, Sheet, Plate, Welded Tube, Wire

Copper

3.9 - 5.0 %

Show Material materials with Copper of 3.9 - 5.0 %

T4511

EN 573-3, EN 754, EN 755

Tube, Profile, Rod, Strip, Sheet, Plate, Welded Tube, Wire

Iron

0.5 %

Show Material materials with Iron of 0.5 %

T4511

EN 573-3

Tube, Profile, Rod

0.50 %

Show Material materials with Iron of 0.50 %

T4511

EN 573-3, EN 754, EN 755

Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire

Magnesium

0.2 - 0.8 %

Show Material materials with Magnesium of 0.2 - 0.8 %

T4511

EN 573-3, EN 754, EN 755

Tube, Profile, Rod, Strip, Sheet, Plate, Welded Tube, Wire

Manganese

0.4 - 1.2 %

Show Material materials with Manganese of 0.4 - 1.2 %

T4511

EN 573-3, EN 754, EN 755

Tube, Profile, Rod, Strip, Sheet, Plate, Welded Tube, Wire

Nickel

0.1 %

Show Material materials with Nickel of 0.1 %

T4511

EN 573-3, EN 754, EN 755

Tube, Profile, Rod, Strip, Sheet, Plate, Welded Tube, Wire

Silicon

0.5 - 0.9 %

Show Material materials with Silicon of 0.5 - 0.9 %

T4511

EN 573-3, EN 754, EN 755

Tube, Profile, Rod, Strip, Sheet, Plate, Welded Tube, Wire

Titanium

0.15 %

Show Material materials with Titanium of 0.15 %

T4511

EN 573-3, EN 754, EN 755

Tube, Profile, Rod, Strip, Sheet, Plate, Welded Tube, Wire

Zinc

0.25 %

Show Material materials with Zinc of 0.25 %

T4511

EN 573-3, EN 754, EN 755

Tube, Profile, Rod, Strip, Sheet, Plate, Welded Tube, Wire

Technological properties

Property
Workability

Moderate Workability